Product details
Product Details
6x19 locked coil wire rope is available with FC (fiber core) and IWRC (independent wire rope core), offering excellent breaking load characteristics and a wide range of applications. For applications requiring higher abrasion resistance, 6x19 locked coil wire rope is more suitable than other 6x19 wire ropes.
Surface treatment: bright or galvanized
Standard: National Standard GB/T 20118-2006
Engineering Applications
Drilling line
Elevator hoist rope
Wire rope slings
Luffing rope
Hoist rope
Crane rope
Sand line, core line and swabbing line
Trawling / ocean sweeping
Ground rope / ground drag rope
Oil well / oilfield
Excavator rope / scraper rope
Fishing line
Tow rope
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 10 | 0.36 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.43 | 70.7 | 7209 | 78.3 | 7982 |
| 12 | 0.52 | 84.1 | 8579 | 93.1 | 9500 |
| 13 | 0.61 | 98.7 | 10068 | 109 | 11149 |
| 14 | 0.7 | 115 | 11677 | 127 | 12930 |
| 16 | 0.92 | 150 | 15252 | 166 | 16889 |
| 18 | 1.16 | 189 | 19303 | 210 | 21375 |
| 20 | 1.44 | 234 | 23831 | 259 | 26389 |
| 22 | 1.74 | 283 | 28835 | 313 | 31931 |
| 24 | 2.07 | 336 | 34317 | 373 | 38000 |
| 26 | 2.43 | 395 | 40274 | 437 | 44598 |
| 28 | 2.82 | 458 | 46709 | 507 | 51723 |
| 30 | 3.23 | 526 | 53620 | 582 | 59376 |
| 32 | 3.68 | 598 | 61008 | 662 | 67557 |
| 34 | 4.15 | 675 | 68872 | 748 | 76265 |
| 36 | 4.65 | 757 | 77213 | 838 | 85501 |
| 38 | 5.18 | 843 | 86030 | 934 | 95265 |
| 40 | 5.74 | 935 | 95235 | 1035 | 105557 |
| 42 | 6.33 | 1030 | 105095 | 1141 | 116377 |
General Engineering Wire Rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive to achieve a high level of performance to extend service life, thereby improving end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimble eyes, swaged ends and wedge sockets, as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and conform to ISO9001.
Selection Guide
During selection, you can confirm the required diameter, nominal tensile strength grade, surface finish (bright or galvanized) and whether configurations such as fiber core (FC) or independent wire rope core (IWRC) are needed according to the actual working conditions. Load performance varies with different core types and strength grades. Welcome to contact us for detailed specifications and quotations.
Product Advantages
This product conforms to the GB/T 20118-2006 standard and adopts a sealed structure design, making it more adaptable than other 6x19 wire ropes in applications requiring higher wear resistance. Bright or galvanized surface finishes can meet the needs of different environments. Welcome to contact us for specific configurations and application recommendations.
Inquiry Guide
To confirm specifications, core type, surface finish and other configurations, welcome to contact us for detailed specifications and quotations. We will provide corresponding selection recommendations and technical support based on your application scenario.
Operating Environment
- In offshore and shipboard settings, this LM Sealed Wire Rope GB6X19(9/9/1) FC is exposed to salt-laden air and seawater spray; the sealed construction and galvanized surface treatment help resist corrosion in such marine atmospheres.
- On construction and crane sites, the rope operates outdoors across wide seasonal temperature swings and varying humidity, where the fiber core maintains flexibility and the locked coil outer layer resists abrasion from sheaves and drums.
- In industrial plants and elevator shafts, the rope runs indoors or in semi-enclosed spaces with moderate humidity; regular lubrication and inspection are recommended to sustain performance in these less aggressive conditions.
- For trawling and ocean sweeping, the rope is deployed in continuous saltwater immersion and repeated wet-dry cycling, making the galvanized option suitable where enhanced corrosion protection is required.