Product Category

LM Rotation Resistant Wire Rope GB19X7 (6/1)


Contact us for a quotation

Product details

Product Details

Includes the three commonly used specifications 17X7, 18X7 and 19X7. To further enhance flexibility and other performance characteristics, we can also supply the specifications 32X7, 35X7 and 37X7.

Surface finish: bright or galvanized

Standard: GB/T 20118-2006

Engineering Applications

  • Offshore crane wire rope

  • Deck crane wire rope

  • Pillar crane wire rope

  • Lifting slings

  • Main hoist wire rope

  • Slings

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Diameter

Weight

 (1770Mpa) 

 (1770Mpa) 

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

50.114.5148016.11639
60.1420.9213123.12360
80.2637.2378941.14196
100.458.1592164.36557
120.5883.6852792.69442
130.6898.11000710911081
140.791141160612612852
161.031491515916516786
181.31881918620821245
201.62322368625726229
221.942812866131131737
242.313343410937037770
262.713924003043544327

General engineering wire rope

 Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5 mm to 64 mm, covering 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.

Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets as well as many other assembly components. We also offer customization services, and our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with the ISO9001 standard.


Selection Guide

Common specifications of LM rotation-resistant wire rope are 17×7, 18×7 and 19×7; for greater flexibility, structures such as 32×7, 35×7 and 37×7 can be considered. When selecting, please match the diameter, breaking load requirements and surface finish (bright or galvanized) to the actual working conditions. Contact us for detailed specifications and quotations, and we will assist you in confirming a suitable model.

Product Advantages

This series of wire rope complies with the GB/T 20118-2006 standard, and its rotation-resistant performance helps reduce kinking and spinning during lifting. The products are suitable for offshore cranes, deck lifting, pillar cranes and main hoisting applications, and are available with bright or galvanized surface finishes. To learn about performance differences among specifications, please contact us for further information.

Inquiry guidance

For the latest data on specific diameters, breaking loads, weights and other parameters, or to confirm availability of specifications such as 32×7, 35×7 and 37×7, please contact us directly. We can recommend a suitable construction based on your working conditions and provide detailed specifications and quotations. Inquiries are welcome, and we will reply as soon as possible.

Operating Environment

  • Rotation-resistant wire rope of the 17X7 / 18X7 / 19X7 family, and the 32X7 / 35X7 / 37X7 specifications, is used on offshore crane wire rope, deck crane wire rope, pillar crane wire rope, main hoist wire rope, lifting slings and slings, so it must be selected for outdoor marine and dock-side service where salt-laden air and continuous load cycling are present.
  • In these lifting duties the rope is exposed to atmospheric humidity and moisture; the bright finish is normally chosen for dry, sheltered reeving, while the galvanized finish is supplied for humid or intermittently wet crane and sling applications.
  • Because the same rope serves cranes and slings, operating conditions also include abrasive contact with sheaves and drums and repeated bending over them; correct groove and drum matching, plus a suitable lubricant, supports performance in these conditions.
  • For service in strongly corrosive media or at temperature extremes, confirm the duty with us before ordering, since the GB/T 20118-2006 standard covers the rope construction rather than a specific site environment.