LM Compacted Non-rotating Wire Rope GB19X7 (6/1)
Product details
Product Details
The 19x7 compacted non-rotating wire rope is available in both galvanized and non-galvanized versions, and there are also 17x7 and 18x7 specifications. To further improve flexibility and other performance characteristics, we also offer specifications such as 32X7, 35X7 and 37X7.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
Engineering Applications
Offshore crane wire rope
Deck crane wire rope
Pillar crane wire rope
Lifting slings
Main hoist wire rope
Sling
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.63 | 91.7 | 9349 | 102 | 10388 |
| 13 | 0.74 | 108 | 10972 | 120 | 12191 |
| 14 | 0.86 | 125 | 12725 | 139 | 14139 |
| 15 | 0.99 | 143 | 14608 | 159 | 16231 |
| 16 | 1.13 | 163 | 16621 | 181 | 18467 |
| 18 | 1.43 | 206 | 21035 | 229 | 23373 |
| 20 | 1.76 | 255 | 25970 | 283 | 28855 |
| 22 | 2.13 | 308 | 31423 | 342 | 34915 |
| 24 | 2.53 | 367 | 37396 | 407 | 41551 |
| 26 | 2.97 | 430 | 43889 | 478 | 48765 |
| 28 | 3.45 | 499 | 50901 | 554 | 56556 |
| 30 | 3.96 | 573 | 58432 | 637 | 64924 |
General engineering wire rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 in various specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must have resistance to crushing, bending fatigue and wear. All our wire ropes strive to achieve a high level of performance to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged ends and wedge sockets, as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.
Selection Guide
When selecting, first clarify the rated load of the lifting equipment, the pulley and drum diameters, the operating environment (such as offshore, humid or corrosive conditions) and the required safety factor, then determine the suitable specification by referring to the diameter and minimum breaking load comparison table. Different surface treatments (bright or galvanized) and constructions (such as 17x7, 18x7, 32x7, etc.) suit different applications. We recommend informing us of your specific working conditions so our technical staff can help match the right specification.
Product Advantages
This 19x7 compacted non-rotating wire rope uses a compacting process and has a tight structure, offering good anti-rotation performance during lifting and hoisting, which helps reduce load swing. The product can be supplied with bright or galvanized surface treatment as required and complies with GB/T 20118-2006, making it suitable for offshore cranes, deck cranes, pillar cranes and main hoisting applications.
Inquiry Guidance
For specific specifications and quotations covering different diameters, surface treatments, and 1770 MPa or 1960 MPa strength grades, please contact us for detailed technical documents and commercial proposals. We can recommend a suitable construction based on your working conditions and confirm supply and delivery arrangements.