Product details
Product Details
6x36 wire rope is available with FC (fiber core) or IWRC (independent wire rope core), and is a general-purpose flexible engineering wire rope. This wire rope offers excellent breaking load capacity and good fatigue resistance, with a long service life and wide application.
Surface finish: bright, Galvanized or 16 marine-grade stainless steel or galvanized
Standard: GB/T 20118-2006
Engineering Applications
General engineering applications
Grab crane ropes
Wire rope slings
Crane ropes
Slings
Winch ropes
Lifeboat ropes
Mooring ropes
Search ropes
Luffing ropes
- Traction ropes
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.26 | 40.3 | 4113 | 44.7 | 4555 |
| 9 | 0.33 | 51 | 5206 | 56.5 | 5764 |
| 10 | 0.41 | 63 | 6427 | 69.8 | 7117 |
| 11 | 0.5 | 76.2 | 7776 | 84.4 | 8611 |
| 12 | 0.59 | 90.7 | 9255 | 101 | 10248 |
| 13 | 0.69 | 107 | 10862 | 118 | 12028 |
| 14 | 0.8 | 124 | 12597 | 137 | 13949 |
| 16 | 1.05 | 161 | 16453 | 179 | 18219 |
| 18 | 1.33 | 204 | 20824 | 226 | 23059 |
| 19 | 1.48 | 228 | 23202 | 252 | 25692 |
| 20 | 1.64 | 252 | 25708 | 279 | 28468 |
| 22 | 1.98 | 305 | 31107 | 338 | 34447 |
| 24 | 2.36 | 363 | 37020 | 402 | 40994 |
| 26 | 2.77 | 426 | 43448 | 472 | 48111 |
| 28 | 3.21 | 494 | 50389 | 547 | 55798 |
| 30 | 3.68 | 567 | 57845 | 628 | 64054 |
| 32 | 4.19 | 645 | 65814 | 715 | 72879 |
| 34 | 4.73 | 728 | 74298 | 807 | 82274 |
| 36 | 5.3 | 817 | 83296 | 904 | 92238 |
| 38 | 5.91 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.54 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.22 | 1112 | 113376 | 1231 | 125546 |
| 44 | 7.92 | 1220 | 124431 | 1351 | 137788 |
General Engineering Wire Rope
Greenlogy TEC LM specializes in supplying multi-strand bright or galvanized steel wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and abrasion. All our wire ropes are engineered to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged ends and wedge sockets, as well as many other assembly components. We also offer custom services: our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and compliant with ISO9001.
Selection Guide
This product is available with FC and IWRC core types, and the surface can be bright, galvanized or otherwise treated to suit different working conditions. Please select based on load requirements, operating environment and matching sheave diameter, among other factors. Contact us for detailed specifications and a quotation.
Product Advantages
The 6x36 construction combines flexibility with fatigue resistance and offers strong breaking load capacity, making it suitable for lifting and hoisting applications involving frequent bending. Core type and surface treatment can be matched to application requirements to suit different working conditions.
Inquiry Guide
If you need a specific diameter, core type, surface treatment or length, please contact us with your application and requirements. We will help confirm the suitable specification and provide a quotation.