Product Category

LM (Coating) Sealed Comp. Wire Rope GB6X19 (9/9/1) FC


Contact us for a quotation

Product details

Product Details

The core of 6X19 compacted filler wire rope (often referred to as 6x25) includes FC (fiber core) and IWRC (independent wire rope core). 6X19 wire rope can handle loads of 1T-5T and is used as wire rope slings. This construction is widely used in the North Sea oil industry.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Engineering Applications

  • Drilling line

  • Elevator hoisting rope

  • Wire rope slings

  • Luffing wire rope

  • Hoisting rope

  • Crane wire rope


  • Sand line, core line and swabbing line

  • Trawling / ocean sweeping

  • Ground rope / ground drag rope

  • Oil well / oilfield

  • Excavator rope / scraper rope

  • Fishing line

  • Tow rope

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Diameter

Weight

(1770Mpa)

(1770Mpa)

(1960Mpa) 

(1960Mpa) 

mm

kg/m

KN

Kg

KN

Kg

100.3658.4595764.76597
110.4370.7720878.37982
120.5284.1857993.19500
130.6198.71006810911149
140.71141167712712930
160.921501525216616889
181.161891930321021375
201.442342383125926389
221.742832883531331931
242.073363431737338000
262.433954027443744598
282.824584670950751723
303.235265362058259376
323.685986100866267556
344.156756887274876265
364.657577721383885501
385.188438603093495265
405.74935953251035105557
426.3310301050951141116377

General Engineering Wire Rope

   Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply high-quality special wire ropes.

Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with assembly components such as thimbles, swaged terminals and wedge sockets, as well as many others. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.


Selection Guide

When selecting, determine the wire rope diameter, construction and surface treatment (bright or galvanized) according to the load requirements, operating environment (such as corrosion and temperature) and installation method of the actual application. We recommend referring to national standard GB/T 20118-2006, and you are welcome to contact us for detailed specifications and selection support.

Product Advantages

This product adopts a 6X19 compacted strand construction, offering high breaking force and fatigue resistance, while the fiber core (FC) provides good flexibility. The galvanized surface treatment enhances corrosion resistance, making it suitable for a variety of industrial applications.

Inquiry Guide

For detailed technical parameters, prices and delivery times, please contact us at any time. Please provide specific requirements such as diameter, length and surface treatment, and we will provide a professional quotation and solution.