Product Category

Product details

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

50*50*63(mm)

Panel size available:

1225*4000,1225*3660,1225*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):8.3/6.0

Bearing bar center:50

Open Aera:78%

Approx Weight:28.8kgs/m²

Liner load(units:mm)

 Span in (mm)

Load in kn/m of widht (concentrated)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4006.83011.8

Uniform load(units:mm)

 Span in (mm)

Load in kn/sqm (uniformed)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4001.715411.8
6006.87314.9
8002.03516.5

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly. 


Application Scenarios

FRP molded grating 50*50 H63 is commonly used for platforms, walkways, trench covers and stair treads in corrosive or humid environments such as chemical, sewage treatment, marine engineering and electroplating facilities. Its grid structure facilitates drainage, ventilation and light transmission, and is also suitable for maintenance access and operating areas requiring slip resistance and lightweight construction. If your working conditions involve specific media or loads, please contact us for detailed specifications and selection advice.

Selection Guide

Selection should take into account the resin system, grating thickness, mesh size, support span, and the corrosivity and flame-retardant requirements of the service environment. Different resin types vary in chemical resistance, flame retardancy and temperature resistance, and should be matched according to the actual contact media and safety regulations. Please provide your working conditions, and our technical team can assist in confirming suitable specifications and configurations.

Product Advantages

Molded grating is integrally formed from resin and fiberglass, offering lightweight, high strength, corrosion resistance, aging resistance, and electrical insulation with non-magnetic properties. It is easy to install and maintain and has a long service life. The 50*50mm mesh and 63mm thickness balance load-bearing capacity and open area, facilitating media flow and reducing structural dead weight. Specific performance varies with resin formulation and service environment; please inquire for tailored information.

Inquiry Guide

To learn about the detailed specifications, resin options, technical data or commercial terms for FRP molded grating 50*50 H63, please contact us for detailed specifications and quotations. Please provide your application scenario, size requirements and environmental conditions, and we will provide selection support and solution recommendations as soon as possible.

Operating Environment

  • This molded FRP grating (50×50 mesh, 63 mm depth) is built on unsaturated polyester resin — isophthalic, vinyl ester, bisphenol or phenolic types in the customization mold — so it is specified for both indoor and outdoor installations, including open-air walkways, platforms and stair treads exposed to sun and rain.
  • The resin matrix and E-glass fiber reinforcement suit wet and humid service conditions such as wash-down areas, drainage covers and coastal or marine-adjacent sites, where the grating is chosen instead of steel for its corrosion resistance.
  • Acid, alkali and salt-laden atmospheres found in chemical plants, water treatment and electroplating lines are typical duty for this grating; the applicable resin grade (OFR-25, IFR-25, VEFR-25 or phenolic MP-5) is selected according to the specific corrosive medium.
  • For phenolic MP-5 grating, the low-toxicity, high flame-retardant formulation is intended for fire-safety-conscious locations such as tunnels, offshore platforms and enclosed process areas where low smoke and flame spread matter; contact us for the full parameter list and the resin recommendation for your site.