Resin

25%

OFR-25、IFR-25、VEFR-25

Fiberglass

65%

E

Filler

8%

ATH、PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

T3815

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 38mm
Open Area: 38%

Approx Weight (With three-core shoots): 14.2kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

15030045075015003000

Load

4500.250.250.510.761.272.546288
6000.250.510.761.272.294.835021
9000.761.522.293.817.62---3353
12001.783.35.088.38------2503
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

4509501450240048509500

Load

450<0.250.250.250.511.272.5413713
6000.250.511.011.523.056.110297
9001.522.794.327.11------6881
12004.328.3812.7---------4099

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

应用场景

拉挤格栅 T-3815 适用于对承载与耐腐蚀同时有要求的平台、走道、沟盖及操作面,常见于化工、水处理、电力与海洋工程等存在腐蚀介质或潮湿环境的场合。若需确认在具体介质、温度或荷载条件下的适用性,欢迎联系我们沟通工况细节。

选型指导

本产品以拉挤“I”“T”型材作承力条、实心管或棒作连接杆组装而成,选型时建议结合承载跨度、使用环境与树脂体系(如 OFR、IFR、VEFR 或酚醛型)综合判断。不同树脂类型对应不同的阻燃与耐腐蚀表现,欢迎提供工况条件,由我们协助推荐合适的配置。

产品优势

相比传统金属格栅,拉挤格栅具有轻质高强、耐腐蚀、免维护等特点,长期使用不易锈蚀,且便于现场切割与安装。其纵向承力条结构使板材在跨度方向具备良好的承载能力,适合需要频繁检修或长期暴露于腐蚀环境的场所。

询盘引导

如需了解拉挤格栅 T-3815 的详细规格、树脂体系选择及商务条件,欢迎联系我们获取详细规格与报价。请提供使用环境、承载要求与尺寸需求,我们将据此给出针对性的方案与供货信息。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor