Breaking Loads
diameter
| mass
|
Minimum breaking load
|
Minimum breaking load(1570 Mpa)
|
mm | kg/m | kN |
Kg |
| 3 | 0.03 | 5 | 509 |
| 4 | 0.06 | 8.89 | 906 |
| 5 | 0.09 | 13.9 | 1417 |
| 6 | 0.13 | 20 | 2039 |
| 7 | 0.18 | 27.3 | 2783 |
| 8 | 0.24 | 35.6 | 3630 |
| 10 | 0.37 | 55.6 | 5669 |
| 12 | 0.54 | 80 | 8157 |
| 14 | 0.73 | 109 | 11114 |