LM Wire Rope GB6X36 IWRC
Please feel freely to contact with us for new price .
产品详情
6x36 wire rope is a flexible general engineering wire rope available with either FC (fibre core) or IWRC (independent wire rope core). The wire rope has a superior breaking load and a good fatigue life. This wire rope can be used for a wide range of applications.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006
.jpg?access_token=05e18ada-556c-4ebc-9c21-f033a9463fae)
Applications
General engineering
Ropes for grab cranes
Wire rope slings
Crane ropes
Hoist rope
Winch ropes
Lifeboat falls
Mooring ropes
Pursing wires
Luffing ropes
Tow ropes
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.26 | 40.3 | 4113 | 44.7 | 4555 |
| 9 | 0.33 | 51 | 5206 | 56.5 | 5764 |
| 10 | 0.41 | 63 | 6427 | 69.8 | 7117 |
| 11 | 0.5 | 76.2 | 7776 | 84.4 | 8611 |
| 12 | 0.59 | 90.7 | 9255 | 101 | 10248 |
| 13 | 0.69 | 107 | 10862 | 118 | 12028 |
| 14 | 0.8 | 124 | 12597 | 137 | 13949 |
| 16 | 1.05 | 161 | 16453 | 179 | 18219 |
| 18 | 1.33 | 204 | 20824 | 226 | 23059 |
| 19 | 1.48 | 228 | 23202 | 252 | 25692 |
| 20 | 1.64 | 252 | 25708 | 279 | 28468 |
| 22 | 1.98 | 305 | 31107 | 338 | 34447 |
| 24 | 2.36 | 363 | 37020 | 402 | 40994 |
| 26 | 2.77 | 426 | 43448 | 472 | 48111 |
| 28 | 3.21 | 494 | 50389 | 547 | 55798 |
| 30 | 3.68 | 567 | 57845 | 628 | 64054 |
| 32 | 4.19 | 645 | 65814 | 715 | 72879 |
| 34 | 4.73 | 728 | 74298 | 807 | 82274 |
| 36 | 5.3 | 817 | 83296 | 904 | 92238 |
| 38 | 5.91 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.54 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.22 | 1112 | 113376 | 1231 | 125546 |
| 44 | 7.92 | 1220 | 124431 | 1351 | 137788 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时请结合工况确认所需直径、芯型(FC或IWRC)、表面处理(光面或镀锌)及抗拉强度等级。LM 6x36钢丝绳兼具柔韧性与抗疲劳性能,适用于频繁弯曲的起重及牵引场景;如对耐磨或耐腐蚀有更高要求,可考虑镀锌表面。欢迎联系我们,我们将根据您的使用条件提供选型建议。
产品优势
6x36结构配合独立的钢丝绳芯(IWRC),在保持良好柔韧性的同时提供较高的断裂荷载能力,并具有较长的使用寿命。该产品可按国标GB/T 20118-2006生产,适用于抓斗起重机、吊索、绞车及系泊等多种通用工程场景。具体性能参数以实际规格表为准,欢迎来图来样定制。
询盘引导
如需了解LM Wire Rope GB6X36 IWRC的详细规格、表面处理选项及供货方案,欢迎联系我们获取详细规格与报价。请提供所需直径、芯型、强度等级和数量,我们将尽快回复并提供技术支持。
简体中文
English