6x7 wire rope include FC( fiber core) and WSC (wire steel core). Usually,we call WSC as 7x7 .   0.5mm to 2mm is most popular diameter ,and it is flexible .While 6x7diameter is over 6mm,it is strong and hard , wide used in Belt conveyor, ropeway traction, fishery fishing, etc.

Surface treatment:Ungalv  or  Galvanized

Standard:GB/T 20118-2006

绿盟GB钢丝绳6x7

 Applications

  • General engineering application

  • Garage door cables

  • Stay wires

  • Small diameter wire rope slings

  • Standing rigging

  • Hanging signs

  • Catenary wire

  • Fencing rope

  • Ski-lifts

 Breaking Loads



Min Breaking Loads
Min Breaking Loads 
diameterWeight(1770Mpa)
(1770Mpa)
mm
Kg/m
KN
Kg
20.012.35239
30.03
5.29
539
40.06
9.4
959
50.09
14.7
1498
60.13
21.2
2157
70.17
28.8
2937
80.22
37.6
3836
90.27
47.6
4855
100.34
58.8
5993
110.42
71.1
7252
120.51
84.6
8631
140.68
115
11748
160.88
150
15344
181.1
190
19420
201.36
235
23975
221.61
284
29010
241.96
338
34525
262.28
397
40518
282.61
461
46992
302.98
529
53945
323.53
602
61377
364.47
762
77681
405.52
940
95902

General Engineering Ropes

   GREENLOGY TEC(LM) specializes in supplying multiple strands of  ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.

   Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.

选型指导

选择6x7钢丝绳时,需综合考虑负载要求、柔韧性、耐腐蚀性及工作环境等因素。对于需要较高柔韧性的场合,建议选择较小直径或纤维芯(FC)结构;若需更高强度,则可考虑钢丝绳芯(WSC)结构。具体选型参数欢迎联系我们获取详细规格与报价。

产品优势

6x7结构钢丝绳具有较高的破断拉力,柔韧性好,适用于多种工程应用。光面或镀锌表面处理可满足不同防腐需求,严格按照国标GB/T 20118-2006生产,确保质量可靠。如需了解更多产品优势及适用场景,欢迎垂询。

询盘引导

如需获取详细技术参数、价格及交货期等信息,请通过网站联系方式与我们联系。我们的专业团队将根据您的需求提供定制化解决方案。欢迎联系我们获取详细规格与报价。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor