6x19 sealed construction is a wire rope construction with superb breaking load characteristics and is used in a wide range of applications, available with both FC (fibre core) and IWRC (independent wire rope core). For applications that require higher wear resistance, 6x19 sealed wire ropes are more suitable than other 6x19 wire ropes.

Surface treatment:Ungalv  or  Galvanized

Standard:GB/T 20118-2006

LM Sealed Wire Rope GB6X19(9/9/1) FC

Applications

  • Drilling ropes

  • Elevator rope

  • Wire rope slings

  • Derricking ropes

  • Pendant ropes

  • Crane rope


  • Sand, coring and swabbing lines

  • Trawl wraps / Pelagic sweeps

  • Ground cables

  • Oil well / Oil field

  • Excavator rope / Scraper rope

  • Fishing rope

  • Drag ropes

Breaking Loads 

Min Breaking Loads

Min Breaking Loads

Min Breaking Loads

Min Breaking Loads


Diameter

Weight 

(1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

100.3658.4595764.76597
110.4370.7720978.37982
120.5284.1857993.19500
130.6198.71006810911149
140.71151167712712930
160.921501525216616889
181.161891930321021375
201.442342383125926389
221.742832883531331931
242.073363431737338000
262.433954027443744598
282.824584670950751723
303.235265362058259376
323.685986100866267557
344.156756887274876265
364.657577721383885501
385.188438603093495265
405.74935952351035105557
426.3310301050951141116377

General Engineering Ropes

   GREENLOGY TEC(LM) specializes in supplying multiple strands of  ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.

   Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.


选型指导

选型时可根据实际工况确认所需直径、公称抗拉强度等级、表面处理(光面或镀锌)以及是否需要纤维芯(FC)或独立钢丝绳芯(IWRC)等配置。不同芯型与强度等级对应的载荷表现存在差异,欢迎联系我们获取详细规格与报价。

产品优势

该产品符合 GB/T 20118-2006 标准,采用密封结构设计,在需要更高耐磨性的应用场景下相较其他 6x19 钢丝绳更具适应性。光面或镀锌表面处理可满足不同环境的使用需求,欢迎联系我们了解具体配置与适用建议。

询盘引导

如需确认规格、芯型与表面处理等配置,欢迎联系我们获取详细规格与报价。我们将根据您的应用场景提供相应的选型建议与技术支持。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor