LM Marine Grade stainless steel Wire Rope GB6x36 (14/7+7/7/1) IWRC
Please feel freely to contact with us for new price .
Product Details
6x36 is the most flexible of our stainless steel wire ropes. It is available with either FC (fibre core) or IWRC (independent wire rope core) ,having a superior breaking load and a good fatigue life.6x36 stainless steel wire ropes are often used for larger diameter stainless steel slings as well as for general engineering applications.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Marine crane rope
Luffing ropes
Lifeboat falls
Davit ropes
Large diameter stainless steel wire rope slings
Marine/Saltwater environment
Sewage treatment works
Breaking Loads
Diameter
| Weight
|
Min Breaking Loads(1570Mpa)
|
Min Breaking Loads(1570Mpa)
|
mm | kg/m | KN |
Kg |
| 8 | 0.28 | 35.8 | 3651 |
| 9 | 0.35 | 45.3 | 4620 |
| 10 | 0.43 | 55.9 | 5701 |
| 11 | 0.54 | 67.6 | 6895 |
| 12 | 0.62 | 80.5 | 8211 |
| 14 | 0.84 | 110 | 11169 |
| 16 | 1.1 | 143 | 14596 |
| 18 | 1.39 | 181 | 18462 |
| 20 | 1.72 | 224 | 22848 |
| 22 | 2.16 | 271 | 27642 |
| 24 | 2.48 | 322 | 32844 |
| 26 | 2.76 | 378 | 38515 |
| 28 | 3.37 | 438 | 44676 |
| 30 | 3.87 | 503 | 51306 |
| 32 | 4.41 | 572 | 58344 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.