LM (Coating) Sealed Wire Rope GB6X19(9/9/1) IWRC

LM (Coating) Sealed Wire Rope GB6X19(9/9/1) IWRC

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

产品详情

6x19  (coating) sealed construction is a wire rope construction with superb breaking load characteristics and is used in a wide range of applications, available with both FC (fibre core) and IWRC (independent wire rope core). For applications that require higher wear resistance, 6x19 sealed wire ropes are more suitable than other 6x19 wire ropes.

Surface treatment:Ungalv  or  Galvanized

Standard:GB/T 20118-2006

LM (Coating) Sealed Wire Rope GB6X19(9/9/1) IWRC

Applications

  • Drilling ropes

  • Elevator rope

  • Wire rope slings

  • Derricking ropes

  • Pendant ropes

  • Crane rope


  • Sand, coring and swabbing lines

  • Trawl wraps / Pelagic sweeps

  • Ground cables

  • Oil well / Oil field

  • Excavator rope / Scraper rope

  • Fishing rope

  • Drag ropes

Breaking Loads 

Min Breaking Loads

Min Breaking Loads

Min Breaking Loads

Min Breaking Loads


Diameter 

Weight 

(1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

100.463642769.87117
110.4876.2777684.48611
120.5890.7925510110248
130.681071086211812028
140.781241259713713949
150.91421446115716013
161.021611645317918219
181.32042082422623059
201.62522570827928468
221.943053110733834447
242.33633702040240994
262.74264344847248111
283.144945038954755798
303.65675784562864054
324.16456581471572879
344.627287429880782274
365.188178329690492238
385.78910928091008102771
406.410081028351116113874
427.0611121133761231125546

General Engineering Ropes

   GREENLOGY TEC(LM) specializes in supplying multiple strands of  ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.

   Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.


Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor