LM (Coating) Fiber Core Wire Rope GB6X36 FC
Please feel freely to contact with us for new price .
产品详情
6x36 wire rope is a flexible general engineering wire rope available with either FC (fibre core) or IWRC (independent wire rope core). The wire rope has a superior breaking load and a good fatigue life. This wire rope can be used for a wide range of applications.
Surface treatment:Ungalv, Galvanized or Marine Grade Stainless Steel
Standard:GB/T 20118-2006

Applications
General engineering
Ropes for grab cranes
Wire rope slings
Crane ropes
Hoist rope
Winch ropes
Lifeboat falls
Mooring ropes
Pursing wires
Luffing ropes
- Tow ropes
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.24 | 37.4 | 3813 | 41.4 | 4222 |
| 9 | 0.3 | 47.3 | 4825 | 52.4 | 5343 |
| 10 | 0.37 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.44 | 70.7 | 7209 | 78.3 | 7982 |
| 12 | 0.53 | 84.1 | 8579 | 93.1 | 9500 |
| 13 | 0.62 | 98.7 | 10068 | 109 | 11149 |
| 14 | 0.72 | 115 | 11677 | 127 | 12930 |
| 15 | 0.83 | 131 | 13405 | 146 | 14844 |
| 16 | 0.94 | 150 | 15252 | 166 | 16889 |
| 18 | 1.19 | 189 | 19303 | 210 | 21375 |
| 19 | 1.33 | 211 | 21507 | 234 | 23816 |
| 20 | 1.47 | 234 | 23831 | 259 | 26389 |
| 22 | 1.78 | 283 | 28835 | 313 | 31931 |
| 24 | 2.11 | 336 | 34317 | 373 | 38000 |
| 26 | 2.48 | 395 | 40274 | 437 | 44598 |
| 28 | 2.88 | 458 | 46709 | 507 | 51723 |
| 30 | 3.3 | 526 | 53620 | 582 | 59376 |
| 32 | 3.76 | 598 | 61008 | 662 | 67557 |
| 34 | 4.24 | 675 | 68872 | 748 | 76265 |
| 36 | 4.76 | 757 | 77213 | 838 | 85501 |
| 38 | 5.3 | 843 | 86030 | 934 | 95265 |
| 40 | 5.87 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.47 | 1030 | 105095 | 1141 | 116377 |
| 44 | 7.11 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.77 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.46 | 1346 | 137268 | 1490 | 152003 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.