Genius FRP  

Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.

Name

Contect

Type

Resin

25%

OFR-25、IFR-25、VEFR-25

Fiberglass

65%

E

Filler

8%

ATH、PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface

Software - Sample 2 for three columns

Smooth surface

Software - Sample 3 for three columns

Antiskid groove surface

I 4010
Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 50%
Approx Weight (With three-core shoots): 17.8kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

4500.380.581.022.034.067.6216593
6000.951.562.544.578.8917.512959
9003.094.647.7315.530.9---8639
12005.848.8914.729.559.2---6420
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190039007000950019500

Load

4500.851.763.225.637.2512.172325
6001.913.717.5612.916.5---42515
9006.5712.823.3---------18863
120014.5---------------10507

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories

I 4010

应用场景

拉挤格栅 I-4010 适用于对承载与耐腐蚀同时有要求的平台、走道、沟盖及楼梯踏板等场合,常见于化工、水处理、电力和海洋工程等环境。不同树脂体系对应不同介质与温度条件,具体适用性欢迎联系我们结合工况确认。

选型指导

选型时请先明确承载需求、跨距、腐蚀介质与阻燃要求,再据此选择树脂类型与格栅厚度、网格尺寸。表中 OFR、IFR、VEFR 及酚醛等体系在阻燃与耐蚀性上各有侧重,欢迎联系我们获取详细规格与选型建议。

产品优势

拉挤格栅以拉挤 I 型、T 型型材作承重条,实心管或棒作连接杆组装而成,因此纵向承载能力强、刚度高,且重量轻、耐腐蚀、便于切割安装。其表面防滑、维护量低,适合替代金属格栅使用。

询盘引导

如需了解拉挤格栅 I-4010 的详细规格、树脂选项与报价,欢迎联系我们,提供您的工况条件与尺寸需求,我们将为您推荐合适方案。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor