Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---


Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

50.8 50.8 H13

50.8*50.8*13(mm)

Panel size available:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/6.0

Bearing bar center:50.8

Open Aera:82%

Approx Weight:5.8kgs/m²

Liner load

Liner load(units:mm)

Span in (mm)

Load in kn/m of widht (concentrated)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4001.53011.8
6003.92114.9
8008.41216.5
100015.91017.0
Uniform load

Uniform load(units:mm)

Span in (mm)

Load in kn/sqm (uniformed)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4000.415411.8
6001.57314.9
8000.43516.5
10009.92117.0
50.8 50.8 H13

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in: 

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

50.8 50.8 H13
50.8 50.8 H13
50.8 50.8 H13

应用场景

玻璃钢模塑格栅50.8*50.8H13适用于需要防滑、耐腐蚀与承载的走道、平台、地沟盖板及楼梯踏步等场合,常见于化工、水处理、电镀与海上平台等腐蚀性环境。其网格结构利于排水、透光与通风,可根据具体工况选择不同树脂体系。欢迎联系我们说明使用环境,获取适配建议。

选型指导

选型时建议先确认承载需求、跨距、腐蚀介质与阻燃要求,再据此选择树脂类型(如邻苯、间苯、乙烯基或双酚A型)及格栅厚度与网格尺寸。不同树脂体系在耐腐蚀与阻燃性能上各有侧重,需结合实际工况权衡。欢迎联系我们提供工况参数,由技术人员协助选型。

产品优势

模塑格栅采用树脂与玻璃纤维一体成型,具有轻质高强、耐腐蚀、防滑及绝缘等特点,且便于切割安装与后期维护。其网格结构可减少积水和积尘,适合长期处于潮湿或化学腐蚀环境的使用需求。具体性能表现随树脂与纤维配比不同而变化,欢迎联系我们获取详细说明。

询盘引导

如需了解玻璃钢模塑格栅50.8*50.8H13的详细规格、树脂选项、价格与交货安排,欢迎联系我们。请提供使用环境、承载要求与所需数量,我们将据此推荐合适方案并回复报价。支持按图定制与批量采购咨询。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor