玻璃钢模塑格栅38*38H50重负载型

玻璃钢模塑格栅38*38H50重负载型

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38 38 50 Heavy duty

38*38*50(mm)

Panel size available:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):11/9.0

Bearing bar center:38

Open Aera:56%

Approx Weight:42kgs/m²

Liner load

Liner load(units:mm)

 Span in (mm)

Load in kn/m of widht (concentrated)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4009.3197.14
Uniform load

Uniform load(units:mm)

 Span in (mm)

Load in kn/sqm (uniformed)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4002.31007.14
6009.9458.55
38 38 50 Heavy duty

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

38 38 50 Heavy duty
38 38 50 Heavy duty
38 38 50 Heavy duty

应用场景

玻璃钢模塑格栅38*38H50重负载型适用于石油化工、电力、污水处理、海洋工程等行业的操作平台、走道、地沟盖板等需要高承载和耐腐蚀的场合。

其38*38mm网格和50mm厚度设计在提供高强度的同时,保持排水、防滑和通风性能,适合潮湿、易积液或需频繁冲洗的环境。

选型指导

选型时需综合考虑承载要求、跨距、支撑方式及使用环境,根据实际荷载选择合适厚度与网格尺寸。

若需更高耐腐蚀等级,可选用间苯、乙烯基酯或双酚A型树脂;有阻燃需求时,可选择添加阻燃剂的配方。欢迎联系我们获取详细规格与选型建议。

产品优势

本产品以不饱和聚酯树脂为基体,玻璃纤维增强,具有轻质高强、耐腐蚀、抗老化、绝缘及免维护等特性。

模塑成型工艺确保网格尺寸精确、整体性好,表面凹槽设计提供防滑效果,重负载型结构可承受较大集中荷载。

询盘引导

如需了解更多关于玻璃钢模塑格栅38*38H50重负载型的技术参数、定制尺寸或批量采购信息,欢迎联系我们获取详细规格与报价。