玻璃钢模塑格栅38*38H25
Please feel freely to contact with us for new price .
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*38*25(mm)
Panel size available:
1220*4010,1220*3660,1524*4010,
997*3012,915*3050Bidirectional force.
Bearing bar thickness (Top/Bottom):6.4/5.0
Bearing bar center:38
Opea Area:68%
Approx Weight:12.3kg/㎡

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
应用场景
玻璃钢模塑格栅38*38H25广泛应用于化工、石油、电力、污水处理、海洋工程等领域的操作平台、走道、楼梯踏步及地沟盖板。其耐腐蚀、防滑、轻便的特性使其成为潮湿、腐蚀性环境的理想选择。
选型指导
选型时请考虑承载需求、腐蚀环境、防火要求及安装方式。不同树脂类型(如邻苯型、间苯型、乙烯基酯型、双酚A型)和添加剂(如ATH、PR)可提供不同的耐腐蚀和阻燃性能。欢迎联系我们获取详细规格与选型建议。
产品优势
玻璃钢模塑格栅具有优异的耐腐蚀性、高强度、轻质、防滑、绝缘及长使用寿命。其38*38mm网格和25mm厚度设计平衡了承载与开孔率,便于安装和维护。
询盘引导
如需了解更多关于玻璃钢模塑格栅38*38H25的技术参数、价格及定制服务,欢迎联系我们获取详细规格与报价。我们的专业团队将为您提供最适合的解决方案。