Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

25 100 H38 Moltrude

25*100*38(mm)

Panel size available:

1220*3660 Length stress      

Bearing bar thickness (Top/Bottom):15.0/5.0

Bearing bar center:25

Open Aera:62%

Approx Weight:21kgs/m²

25 100 H38 Moltrude

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns


Software - Sample 2 for three columns


Software - Sample 3 for three columns



应用场景

模塑格栅常用于化工、电镀、污水处理、海洋工程等平台的走道、操作面与地沟盖板,也可用于需要防滑、耐腐蚀、轻质承载的工业与市政场合。若您的工况涉及特殊介质或载荷,欢迎联系我们说明使用环境,我们可协助推荐合适的树脂体系与格栅规格。

选型指导

选型时可从承载需求、网格尺寸、厚度、树脂类型及表面形式(如防滑砂面)等方面综合考虑。本产品型号标注为25*100H38仿拉挤,表征其网格与厚度方向的基本结构,具体承载与耐腐蚀性能可结合树脂体系(如邻苯、间苯、乙烯基、酚醛等)确定。欢迎联系我们获取详细规格与报价,以便按您的工况匹配合适方案。

产品优势

FRP模塑格栅由不饱和聚酯树脂与玻璃纤维整体模压成型,具有轻质高强、耐腐蚀、防滑、绝缘及易切割安装等特点,仿拉挤外观兼顾了格栅的整体性与条状视觉。相较于传统金属格栅,其耐化学介质与免维护优势更为突出,适合长期处于潮湿或腐蚀环境的场合。

询盘引导

如需了解本产品可选的树脂类型、网格尺寸、颜色及表面处理等,欢迎联系我们获取详细规格与报价。请提供使用环境、承载要求及所需数量,我们将据此为您推荐合适的格栅方案并安排后续沟通。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor