结构型材-平条
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Riglet | Width*Thickness | Width*Thickness | ||
| FS19 | 19*6.4 | 0.25 | 0.75*0.25 | 0.55 |
| FS30A | 30*3 | 0.18 | 1.18*0.12 | 0.4 |
| FS30B | 30*6.4 | 0.37 | 1.18*0.25 | 0.82 |
| FS35 | 35*8 | 0.54 | 1.38*0.31 | 1.19 |
| FS38 | 38*5 | 0.37 | 1.5*0.2 | 0.82 |
| FS40A | 40*8 | 0.62 | 1.57*0.31 | 1.37 |
| FS40B | 40*10 | 0.79 | 1.57*0.39 | 1.74 |
| FS46B | 46*6.4 | 0.58 | 1.81*0.25 | 1.28 |
| FS50A | 50*2 | 0.25 | 1.97*0.08 | 0.55 |
| FS50B | 50*4 | 0.38 | 1.97*0.16 | 0.84 |
| FS50C | 50*6 | 0.59 | 1.97*0.24 | 1.3 |
| FS50D | 50*8 | 0.76 | 1.97*0.31 | 1.68 |
| FS50E | 50*15 | 1.43 | 1.97*0.59 | 3.15 |
| FS60A | 60*2 | 0.24 | 2.36*0.08 | 0.53 |
| FS60B | 60*4 | 0.48 | 2.36*0.16 | 1.06 |
| FS64 | 64*4.8 | 0.6 | 2.52*0.19 | 1.32 |
| FS70 | 70*4 | 0.55 | 2.76*0.16 | 1.21 |
| FS76 | 76*9.5 | 1.42 | 2.99*0.37 | 3.13 |
| FS100A | 100*10 | 1.95 | 3.94*0.39 | 4.3 |
| FS100B | 100*25 | 4.85 | 3.94*0.98 | 10.7 |
| FS102A | 102*3.2 | 0.63 | 4.02*0.13 | 1.39 |
| FS102B | 102*5 | 0.97 | 4.02*0.2 | 2.4 |
| FS102C | 102*6.4 | 1.3 | 4.02*0.25 | 2.87 |
| FS120 | 120*10 | 2.4 | 4.72*0.39 | 5.29 |
| FS152A | 152*10 | 2.92 | 5.98*0.39 | 6.44 |
| FS152B | 152*20 | 5.9 | 5.98*0.79 | 13 |
| FS190 | 190*15 | 5.42 | 7.48*0.59 | 12 |
| FS280 | 280*10 | 5.32 | 11.02*0.39 | 11.7 |
| FS300 | 300*24 | 14.4 | 11.81*0.94 | 31.8 |
| FS355 | 355*5 | 3.5 | 13.98*0.2 | 7.72 |
| FS555 | 555*5 | 5.4 | 21.85*0.2 | 11.9 |
| FS751 | 751*5 | 7.2 | 29.57*0.2 | 15.9 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Standard color | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Grass green,Yellow, Grey, Orange | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | Grass green,Yellow, Grey | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | Grass green,Yellow, Grey | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-平条适用于对强度与跨度有要求的承载与连接部位,如平台支撑、栏杆扶手、走道格栅边框、设备支架及化工、海洋等腐蚀性环境中的结构构件。其玻璃纤维增强树脂体系在需要绝缘、轻质、耐腐蚀的场合具有实际应用价值。具体工况选型建议结合荷载与介质条件与我们沟通确认。
选型指导
选型时主要考虑宽度、厚度与所需承载能力、支撑跨距及使用环境,表中不同规格对应不同截面惯性矩与重量,可按安装空间与受力方式匹配。若涉及拼接、开孔或与其他FRP构件组合,建议提供图纸或使用条件,欢迎联系我们获取详细规格与选型建议。
产品优势
该平条采用拉挤工艺成型,纤维连续分布,具有较高的纵向强度与刚度,同时具备FRP材料共有的轻质、耐腐蚀、电绝缘与免维护特点,便于切割与现场安装。相比传统金属型材,在腐蚀或电磁敏感环境中可减少锈蚀与维护成本,表面可根据需求提供不同处理方式。
询盘引导
如需确认具体规格、长度、表面处理及包装方式,请提供使用场景与数量需求,我们可根据您的项目条件推荐合适型号。欢迎联系我们获取详细规格与报价,我们将安排专人对接并提供技术支持。

简体中文
English