 FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation. 

Channel steel

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Channel steel

A*B*T1*T2


A*B*T1*T2


C2525*14*3*30.28

1" x 1/2" x 1/8" x 1/8"

0.62
C2626*18*3.2*3.20.3

1" x 11/16" x 1/8" x 1/8"

0.66
C3131*23*4*40.65

5/4" x 15/16" x 3/16" x 3/16"

1.43
C3232*13*3*30.25

5/4" x 1/2" x 1/8" x 1/8"

0.55
C3333*29*4*40.65

5/4" x 19/16" x 3/16" x 3/16"

1.43
C3636*30*4*40.68

3/2" x 5/4" x 3/16" x 3/16"

1.5
C4040*24*3.2*3.20.5

25/16" x 15/16" x 1/8" x 1/8"

1.1
C4545*28*6.4*6.41.07

7/4" x 9/8" x 1/4" x 1/4"

2.36
C5050*14*3.2*3.20.44

2" x 9/16" x 1/8" x 1/8"

0.97
C5252*50*6*61.63

33/16" x 2" x 1/4" x 1/4"

3.59
C7070*30*4.5*4.50.95

11/4" x 5/4" x 3/16" x 3/16"

2.09
C7575*35*5*51.37

3" x 11/8" x 3/16" x 3/16"

3.02
C76A76*22*6.4*6.41.31

3" x 7/8" x 1/4" x 1/4"

2.89
C76B76*38*6.4*6.41.7

3" x 3/2" x 1/4" x 1/4"

3.75
C8080*40*10*102.7

25/8" x 25/16" x 3/8" x 3/8"

5.95
C90A90*35*5*51.49

7/2" x 11/8" x 3/16" x 3/16"

3.28
C90B90*35*8*82.1

7/2" x 11/8" x 5/16" x 5/16"

4.63
C102A102*27*3.2*3.20.91

4" x 1" x 1/8" x 1/8"

2.01
C102B102*29*4.8*4.81.45

4" x 9/8" x 3/16" x 3/16"

3.2
C102C102*30*4*41.2

4" x 19/16" x 3/16" x 3/16"

2.65
C102E102*44*4.8*4.81.65

4" x 7/4" x 3/16" x 3/16"

3.64
C102F102*44*6.4*6.42.1

4" x 7/4" x 1/4" x 1/4"

4.63
C117117*85*5*52.7

37/8" x 27/8" x 3/16" x 3/16"

5.95
C120A120*25*5*51.52

19/4" x 1" x 3/16" x 3/16"

3.35
C120B120*30*5*51.62

19/4" x 19/16" x 3/16" x 3/16"

3.57
C120C120*40*5*51.81

19/4" x 25/16" x 3/16" x 3/16"

3.99
C145145*25*5*51.8

23/4" x 1" x 3/16" x 3/16"

3.97
C150A150*100*6.4*6.44.1

6" x 4" x 1/4" x 1/4"

9.04
C150B150*80*10*105.5

6" x 25/8" x 3/8" x 3/8"

12.13
C152A152*42*4.8*4.82.03

6" x 13/8" x 3/16" x 3/16"

4.48
C152B152*42*6.4*6.42.72

6" x 13/8" x 1/4" x 1/4"

6
C152C152*42*8*83.5

6" x 13/8" x 5/16" x 5/16"

7.72
C152D152*42*9.5*9.53.95

6" x 13/8" x 3/8" x 3/8"

8.71
C152E152*51*9.5*9.54.35

6" x 2" x 3/8" x 3/8"

9.59
C160160*48*8*83.7

25/4" x 15/8" x 5/16" x 5/16"

8.16
C203A203*56*6.4*6.43.68

8" x 9/4" x 1/4" x 1/4"

8.11
C203B203*56*9.5*9.55.34

8" x 9/4" x 3/8" x 3/8"

11.77
C203C203*102*12.7*12.79.2

8" x 4" x 1/2" x 1/2"

20.28
C210A210*55*5*52.95

33/4" x 9/4" x 3/16" x 3/16"

6.5
C210B210*80*5*53.42

33/4" x 25/8" x 3/16" x 3/16"

7.54
C210C210*85*5*53.52

33/4" x 27/8" x 3/16" x 3/16"

7.76
C240A240*72*8*85.7

19/2" x 11/4" x 5/16" x 5/16"

12.57
C240B240*115*5*54.4

19/2" x 9/2" x 3/16" x 3/16"

9.7
C254254*70*12.7*12.78.910" x 11/4" x 1/2" x 1/2"

19.62
C292292*70*12.7*12.79.8

23/2" x 11/4" x 1/2" x 1/2"

21.61
C300300*55*5*53.85

12" x 9/4" x 3/16" x 3/16"

8.49
C310A310*115*5*55.1

49/4" x 9/2" x 3/16" x 3/16"

11.24
C381381*90*10*1010.5

15" x 7/2" x 3/8" x 3/8"

23.15
C436436*90*10*1011.7

69/4" x 7/2" x 3/8" x 3/8"

25.79
C491491*90*12*1214.3

77/4" x 7/2" x 1/2" x 1/2"

31.53
C610610*76*6.4*6.49.2

24" x 3" x 1/4" x 1/4"

20.28
C902902*100*10*1020.6

71/2" x 4" x 3/8" x 3/8"

45.42
C970970*40*10*1019.9

153/4" x 25/16" x 3/8" x 3/8"

43.87

Markets  

Software image and text block

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


应用场景

槽钢类结构型材常用于对强度与耐腐蚀同时有要求的承重与支撑部位,例如平台骨架、走道支撑、设备支架及化工、水处理等腐蚀环境中的结构框架。其截面便于与其他型材组合连接,适合需要大跨度或高强度的场合。具体适用工况请结合实际载荷与环境条件确认。

选型指导

选型时建议先明确使用环境的腐蚀等级、承载要求与安装方式,再据此确定截面规格、壁厚与树脂体系;邻苯型树脂适用于一般防腐工况,强腐蚀或特殊介质环境需另行评估。页面上方列出的是槽钢的截面尺寸与单位重量,可据此进行初步对比。如需针对具体项目的选型建议,欢迎联系我们获取详细规格与报价。

产品优势

该型材以玻璃纤维为增强材料、树脂为基体,经模具加热固化并连续拉挤成型,具有轻质高强、耐腐蚀、绝缘及易加工等特点,适合替代部分传统金属型材以降低维护需求。表面可根据需要做包覆或涂层处理,便于适应不同安装环境。具体性能指标以实际供货技术资料为准。

询盘引导

如需了解槽钢的完整规格表、重量参数、可供长度及表面处理选项,欢迎联系我们获取详细规格与报价。请提供目标截面尺寸、数量、使用环境及交货要求,我们将据此推荐合适方案并安排后续沟通。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor