结构型材-平条(乙烯基)
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Riglet | Width*Thickness | Width*Thickness |
| |
FS19 | 19*6.4 | 0.25 | 3/4" x 1/4" | 0.55 |
FS30A | 30*3 | 0.18 | 19/16" x 1/8" | 0.4 |
FS30B | 30*6.4 | 0.37 | 19/16" x 1/4" | 0.82 |
FS35 | 35*8 | 0.54 | 11/8" x 5/16" | 1.19 |
FS38 | 38*5 | 0.37 | 3/2" x 3/16" | 0.82 |
FS40A | 40*8 | 0.62 | 25/16" x 5/16" | 1.37 |
FS40B | 40*10 | 0.79 | 25/16" x 3/8" | 1.74 |
FS46B | 46*6.4 | 0.58 | 29/16" x 1/4" | 1.28 |
FS50A | 50*2 | 0.25 | 2" x 1/16" | 0.55 |
FS50B | 50*4 | 0.38 | 2" x 3/16" | 0.84 |
FS50C | 50*6 | 0.59 | 2" x 1/4" | 1.3 |
FS50D | 50*8 | 0.76 | 2" x 5/16" | 1.68 |
FS50E | 50*15 | 1.43 | 2" x 9/16" | 3.15 |
FS60A | 60*2 | 0.24 | 19/8" x 1/16" | 0.53 |
FS60B | 60*4 | 0.48 | 19/8" x 3/16" | 1.06 |
FS64 | 64*4.8 | 0.6 | 5/2" x 3/16" | 1.32 |
FS70 | 70*4 | 0.55 | 11/4" x 3/16" | 1.21 |
FS76 | 76*9.5 | 1.42 | 3" x 3/8" | 3.13 |
FS100A | 100*10 | 1.95 | 4" x 3/8" | 4.3 |
FS100B | 100*25 | 4.85 | 4" x 1" | 10.7 |
FS102A | 102*3.2 | 0.63 | 4" x 1/8" | 1.39 |
FS102B | 102*5 | 0.97 | 4" x 3/16" | 2.4 |
FS102C | 102*6.4 | 1.3 | 4" x 1/4" | 2.87 |
FS120 | 120*10 | 2.4 | 19/4" x 3/8" | 5.29 |
FS152A | 152*10 | 2.92 | 6" x 3/8" | 6.44 |
FS152B | 152*20 | 5.9 | 6" x 13/16" | 13 |
FS190 | 190*15 | 5.42 | 15/2" x 9/16" | 12 |
FS280 | 280*10 | 5.32 | 11" x 3/8" | 11.7 |
FS300 | 300*24 | 14.4 | 12" x 15/16" | 31.8 |
FS355 | 355*5 | 3.5 | 14" x 3/16" | 7.72 |
FS555 | 555*5 | 5.4 | 22" x 3/16" | 11.9 |
FS751 | 751*5 | 7.2 | 30" x 3/16" | 15.9 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-平条(乙烯基)适用于对耐腐蚀和强度有要求的平台、走道、护栏、支架等结构场景。乙烯基树脂体系使其在酸性、碱性及潮湿环境中具有较好的耐受性,常用于化工、水处理、海洋工程等领域。具体场景选型建议结合荷载与环境条件咨询我们。
选型指导
选型时需综合考虑荷载要求、跨度、支撑间距、环境腐蚀性及安装方式。平条型材的宽度与厚度规格影响其承载能力,不同树脂体系(如乙烯基)影响耐腐蚀等级。如需针对具体项目推荐合适规格,欢迎联系我们获取技术支持。
产品优势
该平条型材采用拉挤工艺成型,具有轻质高强、耐腐蚀、绝缘无磁、易于切割安装等特点。乙烯基树脂赋予其优于普通聚酯的耐化学性能,适合在苛刻环境中长期使用。表面可进行防滑或涂层处理,满足不同工况需求。
询盘引导
如需了解结构型材-平条(乙烯基)的详细规格、尺寸公差、性能参数及商业条款,欢迎联系我们。我们可根据您的项目需求提供定制化方案与报价。
简体中文
English