拉挤格栅 T-3815
发起询价
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 38mm
Open Area: 38%
Approx Weight (With three-core shoots): 14.2kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 150 | 300 | 450 | 750 | 1500 | 3000 | Load |
| 450 | 0.25 | 0.25 | 0.51 | 0.76 | 1.27 | 2.54 | 6288 |
| 600 | 0.25 | 0.51 | 0.76 | 1.27 | 2.29 | 4.83 | 5021 |
| 900 | 0.76 | 1.52 | 2.29 | 3.81 | 7.62 | --- | 3353 |
| 1200 | 1.78 | 3.3 | 5.08 | 8.38 | --- | --- | 2503 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 450 | 950 | 1450 | 2400 | 4850 | 9500 | Load |
| 450 | <0.25 | 0.25 | 0.25 | 0.51 | 1.27 | 2.54 | 13713 |
| 600 | 0.25 | 0.51 | 1.01 | 1.52 | 3.05 | 6.1 | 10297 |
| 900 | 1.52 | 2.79 | 4.32 | 7.11 | --- | --- | 6881 |
| 1200 | 4.32 | 8.38 | 12.7 | --- | --- | --- | 4099 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating T-3815 is suitable for platforms, walkways, trench covers and operating surfaces that require both load-bearing capacity and corrosion resistance. It is commonly used in chemical, water treatment, power and marine engineering applications where corrosive media or humid environments are present. If you need to confirm its suitability under specific media, temperature or load conditions, please contact us to discuss your operating details.
Selection Guidance
This product is assembled with pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as connecting rods. When selecting, we recommend considering the load-bearing span, service environment and resin system (such as OFR, IFR, VEFR or phenolic) comprehensively. Different resin types offer different flame retardant and corrosion resistance performance. Please provide your operating conditions, and we will assist in recommending a suitable configuration.
Product Advantages
Compared with traditional metal grating, pultruded grating features light weight, high strength, corrosion resistance and low maintenance. It resists rusting during long-term use and is easy to cut and install on site. Its longitudinal load-bearing bar structure gives the panel good load-bearing capacity in the span direction, making it suitable for locations requiring frequent maintenance access or long-term exposure to corrosive environments.
Inquiry Guidance
For detailed specifications, resin system options and commercial terms of Pultruded Grating T-3815, please contact us to obtain detailed specifications and a quotation. Please provide your service environment, load-bearing requirements and size requirements, and we will provide a targeted solution and supply information accordingly.
简体中文