Genius FRP    

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

T1215

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 38mm
Open Area: 12%

Approx Weight (With three-core shoots): 19.6kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

15030045075015003000

Load

450<0.250.250.250.511.021.788791
600<0.250.250.510.761.783.567033
9000.511.021.522.795.3310.74679
12001.272.543.566.112.2---3516
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

4509501450240048509500

Load

450<0.250.250.250.511.021.7819227
6000.250.510.761.022.294.3214396
9001.022.033.055.0810.2---9614
12003.056.19.14---------5758

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

Application Scenarios

Pultruded Grating T-1215 uses pultruded I-shaped and T-shaped profiles as load-bearing bars, with solid tubes or rods as connecting rods. It is suitable for platforms, walkways, trench covers and stair treads where both load-bearing capacity and corrosion resistance are required. In humid or corrosive environments such as chemical, water treatment, electroplating and marine engineering, it can serve as an alternative to traditional metal gratings. For suitability under specific working conditions, please contact us to confirm based on your operating environment.

Selection Guide

When selecting, consider the resin system, load-bearing direction, span and installation method: the resin type must match the corrosion and flame-retardant requirements of the environment, the specification and spacing of the load-bearing bars determine the load capacity, and the connecting rod form affects overall stiffness. Different resin and fiber ratios correspond to different corrosion resistance and flame-retardant performance. We recommend providing the medium used, temperature range and load conditions so that we can assist in recommending a suitable configuration.

Product Advantages

The pultrusion process arranges fibers continuously along the load-bearing direction, giving the product high strength and stiffness in the load-bearing direction, along with the common advantages of FRP materials: lightweight, corrosion-resistant and maintenance-free. The grating surface can be made slip-resistant, it is easy to cut and adjust on site during installation, and it does not rust easily over long-term use. Compared with molded grating, pultruded grating is more suitable for applications with load and span requirements.

Inquiry Guide

For detailed specifications, resin options and supply information for Pultruded Grating T-1215, please contact us to obtain detailed specifications and a quotation. Please provide information such as the operating environment, load requirements, dimensions and quantity, and we will provide targeted recommendations and commercial terms accordingly.