拉挤格栅 I-5015
发起询价
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 38mm
Open Area: 50%
Approx Weight (With three-core shoots): 19.1kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.15 | 0.25 | 0.51 | 1.02 | 1.78 | 3.3 | 21836 |
| 600 | 0.31 | 0.51 | 1.02 | 1.78 | 3.56 | 6.86 | 16385 |
| 900 | 1.02 | 1.52 | 2.54 | 6.08 | 11.9 | 20.9 | 10576 |
| 1200 | 2.89 | 4.56 | 7.84 | 14.9 | 28.4 | --- | 7567 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.25 | 0.51 | 0.96 | 2.27 | 2.97 | 4.56 | 95537 |
| 600 | 0.81 | 1.52 | 2.61 | 4.95 | 6.96 | 12.9 | 53755 |
| 900 | 2.58 | 4.93 | 9.15 | 17.7 | --- | --- | 23164 |
| 1200 | 6.59 | 12.7 | --- | --- | --- | --- | 12422 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating I-5015 is suitable for platforms, walkways, trench covers and equipment operating surfaces with combined requirements for load bearing, corrosion resistance and ventilation/drainage. It is commonly used in corrosive environments such as chemical, water treatment, power and marine engineering. Specific scenario suitability must be evaluated based on load, span and media conditions. Contact us for targeted recommendations.
Selection Guide
When selecting, please confirm the resin system (such as orthophthalic, isophthalic, vinyl ester or phenolic), flame retardancy requirements, grating thickness and load bar spacing, and whether the cross rod type matches your span and load. We can recommend suitable specification combinations based on your operating conditions. Contact us for detailed specifications and quotations.
Product Advantages
With pultruded I-profiles as load bars and solid tubes or rods as cross rods, the product maintains light weight while offering good longitudinal load-bearing capacity and corrosion resistance, and is easy to cut, install and maintain. Anti-slip surface and color options can be configured on request. Contact us to confirm available options.
Inquiry Guide
For detailed specifications of I-5015, resin selection, custom sizes and commercial terms, contact us for detailed specifications and quotations. We will provide selection advice and technical support based on your operating conditions.
简体中文
English