Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 40%
Approx Weight (With three-core shoots): 28.5kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m |
|---|---|---|---|---|---|---|---|
(mm) | 450 | 750 | 1000 | 1500 | 2000 | 2500 | 3000 |
| 450 | 0.09 | 0.15 | 0.2 | 0.3 | 0.4 | 0.5 | 0.6 |
| 600 | 0.21 | 0.35 | 0.47 | 0.71 | 0.94 | 1.18 | 1.42 |
| 900 | 0.72 | 1.2 | 1.65 | 2.45 | 3.22 | 4.02 | 4.83 |
| 1200 | 1.71 | 2.84 | 3.79 | 5.69 | 7.58 | 9.48 | 11.4 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 2000 | 3000 | 4000 | 5000 | 6000 | 8000 |
| 450 | 0.12 | 0.25 | 0.37 | 0.55 | 0.62 | 0.75 | 1.09 |
| 600 | 0.29 | 0.59 | 0.88 | 1.18 | 1.48 | 1.77 | 2.37 |
| 900 | 1.05 | 2.02 | 3.03 | 4.05 | 5.02 | 6 | 8.15 |
| 1200 | 2.37 | 4.74 | 7.11 | 9.48 | 6.86 | 8.23 | 11 |
| 1500 | 4.63 | 9.26 | 13.8 | 18.6 | 11.9 | 14.2 | --- |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded grating I-4020 is commonly used for platforms, walkways, trench covers and various industrial operating surfaces that require both load-bearing capacity and corrosion resistance, and is especially suitable for wet, acid-alkali or washdown environments. If your project involves special media or load conditions, please contact us for detailed specifications and a quotation, and our technical team will help confirm suitability.
Selection Guide
During selection, you can consider factors such as load-bearing requirements, span, corrosion level of the service environment and fire protection requirements, and match them with differences in resin systems (such as OFR-25, IFR-25, VEFR-25) and connection methods. As specific parameters need to be calculated according to the project, please contact us for detailed specifications and a quotation, and we will provide targeted recommendations based on your working conditions.
Product Advantages
This product is assembled with pultruded I-profiles as load-bearing bars and solid tubes or rods as connecting rods. It combines light weight, high strength, corrosion resistance and ease of cutting and installation, with an anti-slip surface and low maintenance cost. For more complete performance descriptions and comparison data, please contact us for detailed specifications and a quotation.
Inquiry Guide
If you are looking for a suitable grating solution for your project, you can tell us the service environment, size requirements and load-bearing requirements so that we can connect quickly. Please contact us for detailed specifications and a quotation, and we will arrange a dedicated person to follow up and provide selection support.
Operating Environment
- Pultruded FRP grating with I-shaped bearing bars and pipe or bar connecting rods is used both indoors and outdoors, where it resists moisture, salt spray and weathering better than untreated steel.
- Its corrosion resistance makes it suited to chemically aggressive areas such as plating and pickling lines, wastewater treatment and pulp and paper plants, where steel grating would corrode.
- Selected resin systems (OFR, IFR, VEFR and phenolic MP-5 grades) support use in wet, humid and fire-sensitive locations; the phenolic type offers low toxicity and high flame retardancy for fire-critical applications.
- Typical applications include walkways, platforms, stair treads and trench covers in process plants and other industrial environments; confirm the resin type and temperature range with us before specifying a site.