拉挤格栅 I-40125
发起询价
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 32mm
Open Area: 40%
Approx Weight (With three-core shoots): 19.8kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.24 | 0.39 | 1.02 | 2.03 | 4.06 | 7.62 | 13808 |
| 600 | 0.82 | 1.14 | 2.54 | 4.83 | 9.4 | 18.8 | 10799 |
| 900 | 2.54 | 4.06 | 6.86 | 13.5 | 27.2 | 54.1 | 7194 |
| 1200 | 7.37 | 10.9 | 18.9 | 36.6 | 73.2 | 146 | 5362 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m |
|---|---|---|---|---|---|---|---|---|---|
(mm) | 300 | 500 | 1000 | 1500 | 2000 | 2500 | 5000 | 10000 | 15000 |
| 600 | 0.16 | 0.27 | 0.55 | 0.82 | 1.09 | 1.37 | 2.73 | 5.47 | 8.2 |
| 800 | 0.49 | 0.82 | 1.63 | 2.45 | 3.27 | 4.08 | 8.17 | --- | --- |
| 1000 | 1.16 | 1.93 | 3.86 | 5.79 | 7.72 | 9.64 | --- | --- | --- |
| 1200 | 2.32 | 3.87 | 7.74 | 11.6 | 15.5 | --- | --- | --- | --- |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating I-40125 is assembled from pultruded I-shaped load-bearing bars and solid tubes or rods as connecting rods, making it suitable for platforms, walkways, trench covers and various industrial operating surfaces that require both load-bearing capacity and corrosion resistance. Its open-gap structure facilitates drainage, chip removal and ventilation, and it is commonly used in humid or corrosive environments such as chemical, electroplating, water treatment and marine engineering. If you need to confirm suitability for your specific working conditions, please contact us.
Selection Guide
Selection can be judged by combining the resin system with the service environment: the phenolic type offers outstanding flame retardancy and is suitable for occasions with high fire safety requirements; the vinyl type performs well in corrosion resistance and is suitable for most acid and alkali media environments. The spacing of load-bearing bars, the form of connecting rods and the overall thickness directly affect load-bearing and stiffness performance. Please contact us for detailed specifications and selection advice.
Product Advantages
The pultrusion process arranges fibers continuously along the load-bearing direction, giving the grating high longitudinal strength and stiffness, while also possessing the common features of FRP materials: lightweight, corrosion-resistant, non-conductive and maintenance-free. The surface can be treated for anti-slip, and it is easy to install and cut, making it suitable to replace metal grating in corrosive environments. Specific performance is subject to actual specifications; please contact us to confirm.
Inquiry Guide
If you would like to know the dimensions and specifications, resin type options, load-bearing capacity and supply information of Pultruded Grating I-40125, please contact us for detailed specifications and a quotation. Please provide the service environment, load-bearing requirements and required dimensions, and we will recommend a suitable solution accordingly.
Operating Environment
- Pultruded FRP grating I-40125 is built for both indoor and outdoor installations, where the pultruded "I"-shaped bearing bars and connecting rods resist moisture and weathering without the corrosion problems of metal grating.
- The vinyl-type (VEFR-25) resin system makes this grating suitable for chemically aggressive surroundings such as processing plants and wastewater areas, where spills, fumes and humid air are present.
- For fire-sensitive locations, the phenolic-type (MP-5) version offers low-toxicity, high flame-retardant performance, making it appropriate where fire safety is a priority.
- Continuous outdoor exposure, temperature swings and wet or damp service conditions are all within the intended working scope of this pultruded FRP grating; contact us for the full parameter list for your specific site conditions.