拉挤格栅 HL-4020

拉挤格栅 HL-4020

价格面议

发起询价


欢迎询价。

Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type 

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

HL4020

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 40%

Approx Weight (With three-core shoots): 70.37kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

(mm)

15030045075015003000450060007500
6000.030.070.090.150.310.60.91.191.5
7500.050.10.170.270.541.091.632.22.74
9000.090.190.270.460.921.842.743.664.58
12000.220.430.771.072.144.296.438.5810.7
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

(mm)

4509501450245048509800145001950024400
6000.030.070.120.190.370.751.121.51.85
7500.090.170.260.430.851.72.573.424.27
9000.170.340.510.851.723.445.146.868.58
12000.541.071.622.695.3610.7---------

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

Application Scenarios

Pultruded Grating HL-4020 uses pultruded profiles as load-bearing bars and solid tubes or rods as connecting rods. It is suitable for platforms, walkways, trench covers and various industrial operating surfaces that require both load-bearing capacity and corrosion resistance. In working conditions involving acid and alkali media, moisture or washdown, FRP material is more conducive to long-term use than metal. For suitability in specific scenarios, you are welcome to contact us to confirm based on your working conditions.

Selection Guide

When selecting, factors such as resin type, grating thickness, load-bearing bar spacing and the corrosion level of the service environment should be considered comprehensively; different resins have different emphases in flame retardancy and corrosion resistance. Please provide your service environment, load requirements and installation method, and we can help recommend a suitable specification combination. For detailed specifications and quotations, you are welcome to contact us.

Product Advantages

Pultruded grating uses pultruded profiles as the load-bearing structure, offering relatively high longitudinal strength and stiffness, while also featuring the common FRP characteristics of light weight, corrosion resistance and easy cutting and installation. The surface can be treated for slip resistance, making it convenient for use in wet or oily environments. For specific performance parameters, you are welcome to inquire by email.

Inquiry Guidance

If you need to know the detailed specifications, resin options, colors and commercial terms of Pultruded Grating HL-4020, you are welcome to contact us. Please provide information such as your service environment, size requirements and quantity, and we will reply as soon as possible with a corresponding solution and quotation.

Operating Environment

  • The pultruded FRP grating is built from pultruded "I" and "T" shaped bearing strips with solid pipe or bar connecting rods, a construction that lets it serve as walkway, platform and stair-tread flooring in industrial plants where moisture and washdown are routine.
  • Because the bearing strips are pultruded FRP rather than steel, the grating is suited to indoor and outdoor installations where the surrounding media are corrosive or chemically aggressive, including areas exposed to acids, alkalis and salt-laden air.
  • With a choice of phenolic, vinyl ester and other flame-retardant resin systems, the grating can be specified for environments where fire safety and low toxicity matter as much as corrosion resistance.