玻璃钢模塑格栅 50*50H13

玻璃钢模塑格栅 50*50H13

价格面议

发起询价


欢迎询价。

Genius FRP

 Fiberglass Reinforced Plastic (FRP) grating is a panel with a certain open area ratio, with unsaturated polyester resin (including isophthalic, phenylene, and phenolphthalein, bisphenol types) as the matrix. 

Name

Content

Type

Resin35%OFR-25,IFR-25,VEFR-25

Fiberglass

33%E
Filler31%ATH,PR
Others1%---

Selection of resin type

Resin type

CodeResin type

Flame retardant performance

Recommended

Application

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardancy, used in applications where fire safety is extremely important

VEFR-25

Vinyl ester type

Oxygen index 28 or above

For severely corrosive environments such as acids, alkalis and solvents

VEFR-10

Vinyl ester type

Oxygen index 35 or above

For applications with high flame retardant requirements and excellent acid and alkali resistance

IFR-25

Isophthalic type

Oxygen index 28 or above

More economical than VEFR type, with excellent acid resistance and moderate resistance to alkalis and solvents

IFGR-30

Isophthalic food grade

Oxygen index 26

Mainly used in meat product and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 or above

General acid and alkali resistant environments

OCR

Orthophthalic type

Oxygen index below 28

More economical than OFR-25, no flame retardant requirement

Type of fiberglass roving selected

Code

Roving type

Recommended applications

E

E-glass roving

For applications requiring higher strength and corrosion resistance

Type of filler selected

CodeFiller type

Recommended applications

ATH

Aluminum hydroxide

For flame retardant, smoke suppressant and corrosion resistant applications

PR

No filler, pure resin

For highly corrosive environments

Software - Sample 1 for three columns

Grooved type
Software - Sample 2 for three columns

Surface-sanded type
Software - Sample 3 for three columns

Gritted type

13mm-50x50-s-6001-2

50*50*13(mm) 

Whole panel size:

1220*4000,1220*3660,

1220*2440,915*3050 

Bidirectional load bearing

Rib wall thickness (top/bottom): 6.0/5.0

Bearing bar center spacing: 50

Open area: 82%

Approximate weight per square meter: 4.8kgs/m²

Linear load (unit: mm)

Span (mm)

Width load (line load) kN per meter

Maximum

Recommended

Surface E1*10^6 N-mm^2/m

4001.53011.8
6003.92114.9
8008.41216.5
100015.91017.0

Uniform load (unit: mm)

Span (mm)

Load (uniform load) kN per square meter

Maximum

Recommended

Surface E1*10^6 N-mm^2/m

4000.415411.8
6001.57314.9
8000.43516.5
10009.92117.0
13mm-50x50-s

Features of molded grating

  1. Corrosion resistant.

  2. High slip resistance.

  3. Good work efficiency.

  4. Low installation cost.

  5. Lightweight, high strength, and easy to cut and install.

  6. Uniform color inside and out, with a wide choice of colors.

  7. Colors can be customized to customer requirements to improve the workplace environment.

  8. Good overall economic benefits.

  9. Excellent designability, flexible and diverse dimensions, and stable dimensions.

Applications

FRP Grating
FRP grating is widely used for floor-standing (industrial) floors, stairs, walkways and platforms.Fiberglass reinforced plastic grating offers many advantages: FRP grating, weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.

FRP Grating
FRP Grating 1
FRP Grating 2

Selection Guide

Before selecting a model, please first confirm the service environment: for highly acidic, alkaline or solvent corrosive conditions, vinyl ester (VEFR) resin is suitable; where high flame retardancy and corrosion resistance are required, VEFR-10 or phenolic (MP-5) type may be chosen; for food processing applications, isophthalic food-grade (IFGR-30) resin is recommended. For fillers, ATH (aluminium hydroxide) suits flame retardancy and smoke suppression requirements, while PR (pure resin) suits highly corrosive conditions; for surface type, grooved, sanded or grit-surfaced options can be selected according to anti-slip and wear resistance needs. If you are unsure of the specific model, please contact us and our technical staff will assist with selection based on your working conditions.

Inquiry Guidance

The resin, fiberglass, filler codes and surface types listed on this page are all optional configurations. For specific specifications, performance parameters and commercial terms, please contact us for detailed specifications and quotations. Please provide information such as service environment, load requirements, dimensions and quantity, and we will recommend suitable models and reply with a supply proposal accordingly.

Operating Environment

  • FRP molded grating (including the 50*50H13 mesh) is designed for both indoor and outdoor service, where it resists degradation from UV exposure and weather.
  • With unsaturated polyester resin matrices such as isophthalic, phenylene, and phenolphthalein/bisphenol types, this grating withstands humid and wet conditions without swelling, making it suitable for wash-down areas and coastal installations.
  • It provides long-term resistance to a wide range of corrosive media, including acids, alkalis, and salts, in chemical processing, wastewater treatment, and marine environments.
  • The grating's flame-retardant formulations (e.g., MP-5 phenolic type with oxygen index up to 80) support use in fire-sensitive indoor spaces.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。