玻璃钢模塑格栅 38*38H20

玻璃钢模塑格栅 38*38H20

价格面议

发起询价


欢迎询价。

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

 Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38*38H20

38*38*20(mm)

Panel size available:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.     

Bearing bar thickness (Top/Bottom):6.0/5.0

Bearing bar center:38

Open Aera:65%

Approx Weight:9.8kgs/m²

Liner load

Liner load(units:mm)

Deflection



kg/m



Limit 

Span
(mm)

75

150

300

450

750

load

3000.250.511.021.522.544470
4500.761.523.304.838.132980
6001.783.817.6211.215.32235
7502.795.5911.417.721.11788
9005.3310.715.421.226.61490
Uniform load

Uniform load(units:mm)

Deflection

kg/m²

Limit 

Span
(mm)

350

500

750

1000

1500

2500

load

300<0.250.250.510.511.021.5229280
4501.021.522.293.054.577.6212981
6003.084.577.119.4012.314.17320
7505.848.89------------4085
9007.16---------------3227
38*38H20

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.

38*38H20
38*38H20
38*38H20

Application Scenarios

FRP molded grating is suitable for platforms, walkways and trench covers in chemical, wastewater treatment, marine engineering and power applications where corrosion resistance and slip resistance are critical. If you need an assessment of suitability for your specific operating conditions, please contact us.

Selection Guidance

During selection, match load requirements and the corrosiveness and flame retardant requirements of the service environment against resin type, grating thickness and mesh size. We can provide selection recommendations based on your operating conditions; please contact us for detailed specifications and a quotation.

Product Advantages

Molded grating is integrally formed from resin and fiberglass, offering light weight, high strength, corrosion resistance, slip resistance and ease of cutting and installation, with different resin systems available to suit different media environments. Actual performance is subject to the specific specifications and test data; please contact us for details.

Inquiry Guidance

To confirm specifications, quantities, delivery and commercial terms, please contact us for detailed specifications and a quotation. We will provide a solution according to your project requirements.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。