 FRP (fiberglass reinforced plastic) grating is a panel with a certain open area ratio; the custom mold uses unsaturated polyester resin (including isophthalic, phenylene, type and phenolphthalein, bisphenol) as the framework. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Raw material introduction

 Resin type

Code

Resin type

Flame retardant performance

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Low toxicity and high flame retardancy, for applications where fire safety is extremely important

VEFR-25

Vinyl ester type

Oxygen index 28 or above

For environments with strong corrosion such as acids, alkalis and solvents

VEFR-10

Vinyl ester type

Oxygen index 35 or above

For applications requiring relatively high flame retardancy as well as excellent acid and alkali resistance

IFR-25

Isophthalic type

Oxygen index 28 or above

More economical than VEFR type, excellent acid resistance, moderate resistance to alkali environments

IFGR-30

Isophthalic food grade

Oxygen index 26

Mainly used in meat product and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 or above

General acid and alkali resistance

OCR

Orthophthalic type

Oxygen index below 28

More economical than OFR-25, for applications without flame-retardant requirements

Type of glass fiber coarse sand selected   

Code

Coarse sand type

Recommended applications

E

Alkali-free coarse sand

Applied in applications requiring higher strength and high corrosion resistance

Type of filler selected   

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

Used in high corrosion resistance applications

Software - Sample 1 for three columns

Grooved type

Software - Sample 2 for three columns

Surface ground type

Software - Sample 3 for three columns

Sand-filled type

13 13 H30

13*13*30(mm)

Panel size:

1220*3660,1220*2440,915*3050 Bidirectional load-bearing.     

Rib wall thickness (top/bottom): 7.5&4.5/6.0

Load bar center-to-center spacing: 13

Open area ratio: 30%

Approximate weight per square meter: 19.5kgs/m²

Software image and text block

Molded grating features:

  1. Corrosion resistant 

  2. High slip resistance 

  3. Good work efficiency 

  4. Low installation cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability


Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.   

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Corrosion-resistant FRP grating product display image

Selection guide

13*13H30 indicates the grating mesh size and thickness combination. When selecting a model, the resin system and fiberglass type must be confirmed according to load requirements, support span and corrosive media. Resin can be selected from orthophthalic, isophthalic, vinyl ester or phenolic types, and fillers can also be selected from ATH flame-retardant and smoke-suppressant or pure resin high-corrosion-resistance options. Please contact us for a suitable configuration based on your working conditions.

Inquiry guide

To confirm the load capacity, surface type (grooved, ground or sand-filled) and applicable resin solution for this specification, please contact us for detailed specifications and a quotation. Please provide the operating environment, load requirements and size requirements, and we will assist you with model selection.