玻璃钢模塑格栅 38*38H38

玻璃钢模塑格栅 38*38H38

价格面议

发起询价


欢迎询价。

Business contact.

Inquiries welcome.

 Genius FRP 

 Fiberglass Reinforced Plastic (FRP) grating is a panel with a certain open area, produced with custom-made molds using unsaturated polyester resin (including isophthalic, phenylene, types and phenanthrenequinone, bisphenol) as the skeleton. 

Selection of Resin Type 
Resin Type

Code

Resin Type

Flame Retardant Performance

Recommended Application

MP-5

Phenolic Type

Oxygen index up to approximately 80

Low toxicity and high flame retardance, for applications where fire safety is extremely important

VEFR-25

Vinyl Type

Oxygen index 28 or above

For severely corrosive environments such as acids, alkalis and solvents

VEFR-10

Vinyl Type

Oxygen index 35 or above

For applications with high flame-retardant requirements as well as excellent acid and alkali resistance

IFR-25

Isophthalic type

Oxygen index 28 or above

More economical than VEFR type, with excellent acid resistance and moderate alkali and solvent resistance

IFGR-30

Isophthalic food grade

Oxygen index 26

Mainly used for meat products and food processing plants

FR-25

Orthophthalic type

Oxygen index 28 or above

General acid and alkali resistance environment

OCR

Orthophthalic type

Oxygen index below 28

More economical than OFR-25, no flame-retardant requirement

Type of fiberglass roving selected

Code

Roving type

Recommended Application

E

E-glass roving

For applications requiring higher strength and corrosion resistance

  Type of filler selected

Code

Filler type

Recommended Application

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing, corrosion-resistant applications

PR

No filler, pure resin

For highly corrosive environments

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

Software image and text block

38*38*38(mm)

Panel size:

1220*4000,1220*3660,1220*2440,

915*3050,1524*3050,

1524*4000 

Bidirectional force. 

Rib thickness (top, bottom): 7.0/5.0

Bearing bar center spacing: 30

Open area: 68%

Approx. weight per square meter: 19.5 kg/㎡ 

Linear load (unit: mm)

Deflcvtion

kg/m


Limit
Span
(mm)
1503004506007501500Load
300
0.360.480.610.760.891.0617116
6000.661.251.852.463.078.488718
9001.803.685.567.429.3013.85817
12004.759.6814.619.621.2---3755

Uniform load (unit: mm)

Deflcvtion


kg/m²


Span
(mm)
2404809801450245036504880
3000.090.190.380.490.781.05---
6000.430.811.552.313.845.74---
9001.703.456.9610.517.523.3---
12005.9712.232.632.638.7------
FRP 38*38*38

Features of molded grating:

  1. Corrosion resistant. 

  2. High anti-slip performance. 

  3. High work efficiency. 

  4. Low installation cost. 

  5. Fire resistant, flame retardant. 

  6. Lightweight, high strength, and easy to cut and install.

  7. Colors can be customized according to customer requirements to improve the production environment.

  8. Good overall economic benefits.

  9. Highly adaptable in design, available in diverse and flexible sizes, dimensionally stable.

Applications

Zhuoyi FRP grating
FRP grating is widely used in industrial floors, stairs, walkways and platforms.FRP grating offers many advantages: weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.

FRP Grating 38*38*38
FRP Grating 38*38*38
FRP Grating 38*38*38

Operating Environment

  • Built for outdoor and indoor industrial service: molded FRP grating such as this 38*38H38 panel is produced with unsaturated polyester resin, so it withstands weathering, UV exposure and moisture without the corrosion that attacks steel grating in open plants, walkways and platforms.
  • Suitable for chemically aggressive surroundings: the resin systems used in this FRP grating (isophthalic, phenylene, bisphenol and related types) are selected for resistance to acids, alkalis, salts and other corrosive media found in chemical, wastewater and processing areas.
  • Flame-retardant resin grades are available for environments where fire performance matters: the phenolic type reaches a high oxygen index, making this grating a fit for areas requiring low-toxicity, high flame-retardant behavior.
  • Works across the temperature and humidity swings typical of plant floors, cooling towers, marine and coastal sites, and wash-down zones; for the recommended resin grade and full parameter list for your specific operating conditions, contact us.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送