结构型材-实心方棒(邻苯)

结构型材-实心方棒(邻苯)

价格面议

发起询价


欢迎询价。

Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Solid square sticks

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Solid square sticks

A*B
A*B
SSR2525*251.231" x 1"2.71
SSR3232*3225/4" x 5/4"4.41
SSR3838*382.83/2" x 3/2"6.17

Markets 

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Solid square rods are suitable for high-strength, large-span structural supports, connectors and various load-bearing frames, especially in construction, bridges and industrial platforms where corrosion resistance and light weight are required. Their smooth surface and stable cross-section also facilitate secondary processing and installation.

Selection Guide

When selecting, please determine the side length and length of the square rod based on structural load, span and environmental conditions, while considering installation methods and connection requirements. We offer a variety of sizes; welcome to contact us for detailed specifications and selection support.

Product Advantages

Made with orthophthalic resin and fiberglass reinforcement, solid square rods offer excellent mechanical properties, corrosion resistance and electrical insulation, and are lightweight and easy to cut and drill. Their smooth surface and stable dimensions make them suitable for engineering projects with high strength and durability requirements.

Inquiry Guide

For specific specifications, prices or customization needs, please contact us for detailed specifications and quotes. Our technical team will provide professional advice based on your project.

Operating Environment

  • These pultruded solid square sticks are suited to both indoor and outdoor installations, where the glass fiber reinforcement and cured resin matrix resist moisture, humidity and weathering far better than untreated steel.
  • Typical service conditions include exposure to mild acids, alkalis, salts and other corrosive media found in chemical plants, water treatment areas and coastal sites; the vinyl ester resin system (邻苯) gives the profile its corrosion resistance in these aggressive settings.
  • Because the material is non-conductive and non-magnetic, the square sticks are also used in environments where electrical insulation or electromagnetic transparency is required, such as near energized equipment or in instrument support frames.
  • Continuous outdoor exposure to UV and temperature cycling does not cause the rust or galvanic corrosion that affects metal profiles, making these structural shapes a practical choice for bridge, walkway and platform applications in all seasons.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送