Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Plum tube

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Plum tube

D1*D2*T
D1*D2*T
CT32A19*32*6.41.110.75*1.26*0.252.45
CT34A19*34*7.51.30.75*1.34*0.32.87
CT32B25*32*3.50.660.98*1.26*0.141.46
CT4229*42*6.41.351.14*1.65*0.252.98
CT45A28*45*8.51.861.1*1.77*0.334.1
CT45B32*45*6.41.11.26*1.77*0.252.43
CT5151*36*71.752.01*1.42*0.283.86
CT90B71*90*9.55.72.8*3.54*0.3712.6

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Standard color

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Grass green,Yellow, Grey, Orange

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

Grass green,Yellow, Grey

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

Grass green,Yellow, Grey

General acid and alkali environment

Application:

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

As a type of structural profile, quincunx tubes are commonly used in frames and support positions requiring light weight, high strength and corrosion resistance, such as platform railings, ladders, supports and structural components in power and chemical environments. If you need to confirm suitability for your specific working conditions, please contact us.

Selection Guidance

During selection, match the cross-sectional dimensions, wall thickness and length according to the load type, span, mounting interface and corrosion resistance requirements. Different specifications vary in load capacity and self-weight. For specific dimensions and selection advice, please contact us for detailed specifications and a quotation.

Product Advantages

Quincunx tubes are pultruded from fiberglass reinforced materials and resin systems, offering a good strength-to-weight ratio, corrosion resistance and electrical insulation properties, making them suitable for replacing some traditional metal profiles. For different resin systems and surface treatment options, please contact us to confirm.

Inquiry Guidance

If you would like to know the available specifications, size range, supply forms and commercial terms of quincunx tubes, please provide your application scenario and required quantity, and we will recommend a suitable solution accordingly. Please contact us for detailed specifications and a quotation.

Operating Environment

  • This pultruded FRP plum tube is a glass fiber reinforced composite with resin as the adhesive and a glass fiber cloth reinforcement layer, so it is suited to both indoor and outdoor installations where moisture and weather exposure are present.
  • The cured FRP section tolerates humid atmospheres and the corrosive media typical of chemical, wastewater and coastal plant environments, where steel profiles would require ongoing protection.
  • Because the tube is formed with a closed plum cross-section, it is typically used as a structural member in high-strength, large-span situations such as industrial walkways, platforms and support frames.
  • For service temperature ranges, chemical exposure conditions or UV requirements in a specific project, contact Greenlogy TEC with your application details so the suitable pultruded profile can be confirmed.