FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.
.png?access_token=fe26106f-1237-434c-93f7-f44049242e94)
Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Skirting board | A*B*T | A*B*T | ||
M2 | 100*13*3.2 M-shape | 1.1 | 4" x 1/2" x 1/8" M-shape
| 2.43 |
M3 | 100*16*5 M-shape | 1.3 | 4" x 5/8" x 3/16" M-shape | 2.87 |
M4 | 148*12*3 M-shape | 1.27 | 23/4" x 1/2" x 1/8" M-shape | 2.8 |
W1 | 100*19*5 W-shape | 1.36 | 4" x 3/4" x 3/16" W-shape | 3 |
W2 | 100*15*3.2 W-shape | 1.1 | 4" x 9/16" x 1/8" W-shape | 2.43 |
W3 | 150*15*3.2 W-shape | 1.6 | 6" x 9/16" x 1/8" W-shape | 3.53 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
This isophthalic structural profile kick plate is suitable for edge protection of platforms, walkways, tank areas and trenches where corrosion resistance and load-bearing are required, providing protection, edge sealing and a decorative function. It is commonly used as a matching component for FRP grating or profiles in chemical, wastewater treatment, electroplating, marine engineering and similar environments. For specific environment suitability, please contact us for detailed specifications and a quotation.
Selection Guide
When selecting a model, the span, load and fixing method of the installation location can be considered together with the A*B*T cross-sectional dimensions and models such as M2, M3 and M4. The isophthalic resin system is suitable for highly corrosive working conditions. If it is to be used together with other FRP profiles or grating, we recommend providing drawings or on-site dimensions. For detailed specifications and a quotation, please contact us.
Product Advantages
Using glass fiber reinforcement and isophthalic resin as the matrix, it is formed through heating, molding, curing and pultrusion, offering good mechanical properties, corrosion resistance and dimensional stability, and is suitable for high-strength, long-span scenarios. The surface can be treated in different ways as required, making installation and maintenance easier. Please contact us for detailed specifications and a quotation.
Inquiry Guide
To confirm the dimensions, color, length and supporting components of this isophthalic kick plate, please let us know your application scenario and required quantity, and we will provide detailed specifications and a quotation. You can also contact us for samples and technical support.
Operating Environment
- This isophthalic resin skirting board is a pultruded FRP structural profile, so it is suited to both indoor and outdoor installation where the base of a wall, platform or walkway edge needs protection.
- The isophthalic polyester resin system gives the profile better resistance to moisture and to splash and spillage of mild chemical media than standard orthophthalic resin, making it a practical choice for wet process areas, wash-down zones and coastal or humid sites.
- As a glass fiber reinforced composite, the skirting board does not corrode like steel and needs no painting, so it keeps its function in damp, salt-laden or lightly aggressive atmospheres.
- Continuous service temperature and resistance to specific chemicals depend on the resin, the medium and the concentration involved; contact us with your site conditions and we will confirm whether this isophthalic profile is the right grade for your project.