FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
H beam | A*B*T1*T2 | A*B*T1*T2 | ||
HB76 | 76*76*6.4*6.4 | 2.67 | 3" x 3" x 1/4" x 1/4" | 5.73 |
HB102A | 102*102*6.4*6.4 | 3.59 | 4" x 4" x 1/4" x 1/4" | 7.91 |
HB102B | 102*102*8*8 | 4.5 |
4" x 4" x 5/16" x 5/16" | 9.92 |
HB152A | 152*152*6.4*6.4 | 5.43 |
6" x 6" x 1/4" x 1/4" | 11.97 |
HB152B | 152*152*9.5*9.5 | 8.1 |
6" x 6" x 3/8" x 3/8" | 17.86 |
HB203A | 203*203*9.5*9.5 | 10.8 |
8" x 8" x 3/8" x 3/8" | 23.81 |
HB203B | 203*203*12.7*12.7 | 14.4 |
8" x 8" x 1/2" x 1/2" | 31.66 |
HB203C | 203*203*6.4*6.4 | 7.5 |
8" x 8" x 1/4" x 1/4" | 16.53 |
HB254A | 254*254*9.5*9.5 | 13.6 |
10" x 10" x 3/8" x 3/8" | 29.98 |
HB254B | 254*254*12.7*12.7 | 18 |
10" x 10" x 1/2" x 1/2" | 39.77 |
HB305 | 305*305*12.7*12.7 | 21.5 |
12" x 12" x 1/2" x 1/2" | 47.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
乙烯基H梁适用于对耐腐蚀与结构强度同时有要求的场合,如化工、水处理、海洋工程、海上平台及各类腐蚀性环境中的承重与支撑结构。其大跨度、高强度的特性也可用于平台走道、设备支架与框架系统。具体工况下的适用性,欢迎联系我们结合实际使用条件进行评估。
选型指导
选型时请先确认截面尺寸(A*B*T1*T2)、跨距、承载方式与所处介质的腐蚀性,再结合安装条件确定连接与固定方案。不同截面规格在刚度与自重上存在差异,需按实际受力状态匹配。若需计算建议与规格对照,欢迎联系我们获取详细规格与报价。
产品优势
产品以玻璃纤维为增强材料、树脂为基体,经浸透、模压加热固化并拉挤成型,具备良好的物理性能与稳定的截面一致性。乙烯基体系在耐腐蚀方面表现突出,同时具有轻质高强、便于切割加工与现场安装的特点。相比传统金属型材,更适用于潮湿与腐蚀性环境中的长期使用。
询盘引导
如需了解乙烯基H梁的规格、尺寸公差、颜色、表面处理及包装运输等商务信息,欢迎联系我们。请提供所需截面、数量与使用环境,我们将据此提供详细规格与报价,并协助确认交付方案。
简体中文
English