FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Flat | Thickness*Width | Thickness*Width | ||
FP32A | 3.2*1000 | 6.18 | 1/8" x 39" | 13.6 |
FP32B | 3.2*1220 | 7.42 | 1/8" x 48" | 16.4 |
FP40A | 4*800 | 6.2 | 3/16" x 32" | 13.7 |
FP40B | 4*1200 | 9.19 | 3/16" x 48" | 20.3 |
FP48 | 4.8*1000 | 9.3 | 3/16" x 39" | 20.5 |
FP50A | 5*440 | 4.25 | 3/16" x 17" | 9.37 |
FP50B | 5*1220 | 11.8 | 3/16" x 48" | 26 |
FP64 | 6.4*1220 | 14.84 | 1/4" x 48" | 32.7 |
FP95 | 9.5*1220 | 22.02 | 3/8" x 48" | 48.6 |
FP127 | 12.7*1220 | 29.44 | 1/2" x 48" | 64.9 |
FP160 | 16*1220 | 37.2 | 5/8" x 48" | 82 |
FP190 | 19*1220 | 44.1 | 3/4" x 48" | 97.2 |
FP254 | 25.4*1220 | 59 | 1" x 48" | 130 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
This structural profile flat panel is suitable for platforms, walkways, handrails, support beams and various load-bearing structural components that require strength, span and corrosion resistance. It can also be used as a structural alternative in corrosive environments such as chemical, marine and wastewater treatment applications. For load and span matching in specific scenarios, please contact us to discuss based on your actual working conditions.
Selection Guide
When selecting, first confirm the thickness and width specifications, then evaluate the required cross-sectional dimensions based on the load, span and corrosion conditions of the operating environment. The specifications listed in the table cover common flat panel sizes. If the existing specifications do not fully match your needs, please contact us for detailed specifications and selection recommendations.
Product Advantages
Made from glass fiber reinforcement with a resin matrix through the pultrusion process, it offers good physical properties and corrosion resistance, suitable for high-strength, long-span applications and situations where traditional materials are prone to corrosion. Compared with metal materials, it is lighter in weight, making transportation and installation easier. For specific performance parameters, please contact us for detailed information.
Inquiry Guide
For detailed specifications, pricing, supply capability and other commercial terms of this structural profile flat panel, please contact us for details and a quotation. Our team will provide corresponding support based on your application requirements.
简体中文
English