Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Riglet | Width*Thickness | Width*Thickness | ||
| FS19 | 19*6.4 | 0.25 | 0.75*0.25 | 0.55 |
| FS30A | 30*3 | 0.18 | 1.18*0.12 | 0.4 |
| FS30B | 30*6.4 | 0.37 | 1.18*0.25 | 0.82 |
| FS35 | 35*8 | 0.54 | 1.38*0.31 | 1.19 |
| FS38 | 38*5 | 0.37 | 1.5*0.2 | 0.82 |
| FS40A | 40*8 | 0.62 | 1.57*0.31 | 1.37 |
| FS40B | 40*10 | 0.79 | 1.57*0.39 | 1.74 |
| FS46B | 46*6.4 | 0.58 | 1.81*0.25 | 1.28 |
| FS50A | 50*2 | 0.25 | 1.97*0.08 | 0.55 |
| FS50B | 50*4 | 0.38 | 1.97*0.16 | 0.84 |
| FS50C | 50*6 | 0.59 | 1.97*0.24 | 1.3 |
| FS50D | 50*8 | 0.76 | 1.97*0.31 | 1.68 |
| FS50E | 50*15 | 1.43 | 1.97*0.59 | 3.15 |
| FS60A | 60*2 | 0.24 | 2.36*0.08 | 0.53 |
| FS60B | 60*4 | 0.48 | 2.36*0.16 | 1.06 |
| FS64 | 64*4.8 | 0.6 | 2.52*0.19 | 1.32 |
| FS70 | 70*4 | 0.55 | 2.76*0.16 | 1.21 |
| FS76 | 76*9.5 | 1.42 | 2.99*0.37 | 3.13 |
| FS100A | 100*10 | 1.95 | 3.94*0.39 | 4.3 |
| FS100B | 100*25 | 4.85 | 3.94*0.98 | 10.7 |
| FS102A | 102*3.2 | 0.63 | 4.02*0.13 | 1.39 |
| FS102B | 102*5 | 0.97 | 4.02*0.2 | 2.4 |
| FS102C | 102*6.4 | 1.3 | 4.02*0.25 | 2.87 |
| FS120 | 120*10 | 2.4 | 4.72*0.39 | 5.29 |
| FS152A | 152*10 | 2.92 | 5.98*0.39 | 6.44 |
| FS152B | 152*20 | 5.9 | 5.98*0.79 | 13 |
| FS190 | 190*15 | 5.42 | 7.48*0.59 | 12 |
| FS280 | 280*10 | 5.32 | 11.02*0.39 | 11.7 |
| FS300 | 300*24 | 14.4 | 11.81*0.94 | 31.8 |
| FS355 | 355*5 | 3.5 | 13.98*0.2 | 7.72 |
| FS555 | 555*5 | 5.4 | 21.85*0.2 | 11.9 |
| FS751 | 751*5 | 7.2 | 29.57*0.2 | 15.9 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Standard color | Recommended usage occasions |
|---|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Grass green,Yellow, Grey, Orange | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | Grass green,Yellow, Grey | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | Grass green,Yellow, Grey | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
The structural flat bar is suitable for load-bearing and connecting parts that require strength and span, such as platform supports, handrails, walkway grating frames, equipment supports, and structural components in corrosive environments such as chemical and marine applications. Its glass fiber reinforced resin system has practical application value in situations requiring insulation, light weight, and corrosion resistance. For selection under specific working conditions, we recommend communicating with us to confirm based on load and medium conditions.
Selection Guidance
When selecting, mainly consider width, thickness, required load-bearing capacity, support span, and service environment. Different specifications in the table correspond to different moments of inertia and weights, which can be matched according to installation space and loading condition. If splicing, openings, or combination with other FRP components are involved, we recommend providing drawings or usage conditions. Please contact us for detailed specifications and selection advice.
Product Advantages
This flat bar is formed by the pultrusion process with continuous fiber distribution, offering high longitudinal strength and stiffness. It also has the common FRP characteristics of light weight, corrosion resistance, electrical insulation, and maintenance-free operation, and is easy to cut and install on site. Compared with traditional metal profiles, it can reduce rust and maintenance costs in corrosive or electromagnetically sensitive environments. Different surface treatments can be provided according to requirements.
Inquiry Guidance
To confirm specific specifications, length, surface treatment, and packaging method, please provide your application scenario and quantity requirements. We can recommend suitable models based on your project conditions. Please contact us for detailed specifications and quotations. We will arrange dedicated personnel to follow up and provide technical support.
Operating Environment
- This pultruded FRP flat strip is built for both indoor and outdoor service, where the glass fiber reinforcement and resin matrix resist moisture and humidity without swelling or rusting.
- In industrial plants and chemical processing areas, the flat strip withstands exposure to corrosive media such as acids, alkalis and salts, making it suitable for environments where steel would degrade.
- As a structural profile for high-strength, large-span situations, it performs across a wide temperature range without losing dimensional stability.
- Typical installations include walkways, platforms and support frames where the flat strip is exposed to weather, washdown or chemical splash.