拉挤格栅 T-3320
发起询价
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 33%
Approx Weight (With three-core shoots): 20.27kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 600 | --- | 0.25 | 0.51 | 1.02 | 1.78 | 3.3 | 16876 |
| 900 | 0.51 | 0.76 | 1.27 | 2.29 | 4.57 | 9.4 | 7492 |
| 1200 | 1.02 | 1.52 | 2.29 | 4.83 | 9.91 | 19.6 | 4215 |
| 1500 | 1.78 | 2.79 | 4.57 | 9.14 | 18.3 | 36.6 | 2696 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 600 | 0.25 | 0.51 | 0.76 | 1.52 | 2.03 | 4.06 | 55368 |
| 900 | 0.76 | 1.52 | 3.05 | 5.59 | 7.73 | 15 | 36895 |
| 1200 | 2.29 | 4.57 | 9.4 | --- | --- | --- | 27659 |
| 1500 | 5 | 9.91 | --- | --- | --- | --- | 22137 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating T-3320 is suitable for industrial platforms, walkways, trench covers and equipment operating surfaces where load-bearing capacity and corrosion resistance are required. If your working conditions involve specific media, temperature or load requirements, please contact us to discuss your specific operating environment.
Selection Guide
When selecting, factors such as resin type (e.g. orthophthalic, isophthalic, vinyl ester or phenolic), load bar specifications, grating thickness and mesh size, as well as installation support span, should be considered comprehensively. Please share your operating environment and load requirements with us, and we will assist you in confirming a suitable configuration.
Product Advantages
Pultruded grating uses pultruded profiles as load bars, offering high longitudinal strength and stiffness, light weight, corrosion resistance, easy cutting and installation, and reduced maintenance requirements. Compared with traditional metal grating, it is more adaptable in humid, acid and alkali corrosive environments.
Inquiry Guide