拉挤格栅 T-3310
发起询价
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 33%
Approx Weight (With three-core shoots): 11.2kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.58 | 0.86 | 1.45 | 2.87 | 5.74 | --- | 10309 |
| 600 | 1.27 | 1.93 | 3.23 | 6.45 | --- | --- | 7731 |
| 900 | 4.01 | 5.99 | 10.1 | --- | --- | --- | 5024 |
| 1200 | 8.99 | --- | --- | --- | --- | --- | 3620 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.56 | 1.07 | 2.13 | 4.04 | 5.23 | --- | 45076 |
| 600 | 1.63 | 3.23 | 6.54 | 12.1 | --- | --- | 25363 |
| 900 | 7.52 | 15 | --- | --- | --- | --- | 10971 |
| 1200 | --- | --- | --- | --- | --- | --- | 5938 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating T-3310 is suitable for platforms, walkways, trench covers, stair treads and equipment operating surfaces that require a combination of load-bearing capacity, corrosion resistance, and ventilation and drainage. It is commonly used in chemical, water treatment, electroplating, marine engineering and power applications where damp, acid, alkali or salt spray environments exist. If your operating conditions involve high temperatures, severe corrosion or special loads, please contact us to confirm a suitable solution based on the specific media, span and installation method.
Selection Guide
When selecting, we recommend first clarifying the resin system (such as OFR, IFR, VEFR or phenolic types, corresponding to different flame retardant and corrosion resistance orientations), the load-bearing direction and the support span, then confirming the grating thickness, mesh spacing and connection method to match the actual load and installation conditions. Since different resin and fiber ratios affect strength, flame retardancy and corrosion resistance, please contact us with your operating parameters and we will assist you in completing the selection and specification confirmation. For detailed specifications and quotations, please contact us.
Product Advantages
Pultruded Grating T-3310 uses pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars, combined with solid tubes or rods as connecting rods, assembled according to a certain process with gaps retained in the panel surface, thus combining relatively high longitudinal load-bearing capacity with light weight, corrosion resistance, and ease of cutting and installation. This structure facilitates ventilation, drainage and light transmission, and is non-conductive and non-magnetic, making it suitable as a replacement for some metal gratings in corrosive environments. Specific performance varies with resin and fiber configuration; please contact us to confirm the applicable configuration.
Inquiry Guide
For further information on the detailed specifications, resin selection recommendations and commercial terms of Pultruded Grating T-3310, please contact us and provide your operating environment, load-bearing requirements and size requirements, and we will provide a targeted solution and quotation accordingly. Please contact us for detailed specifications and quotations.