  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

HL6020

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 60%

Approx Weight (With three-core shoots): 43.5kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

(mm)

15030045075015003000450060007500
6000.050.10.130.230.460.891.351.782.24
7500.080.150.250.40.811.632.443.284.09
9000.130.280.410.691.372.744.095.466.83
12000.330.640.971.63.26.49.612.816
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

(mm)

4509501450245048509800145001950024400
6000.050.10.180.280.561.121.682.242.77
7500.130.250.380.641.272.553.845.116.38
9000.250.510.761.272.575.137.6710.212.8
12000.811.62.414.01816---------

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

Application Scenarios

Pultruded grating is assembled with pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as cross rods. It is suitable for platforms, walkways, trench covers and equipment operating surfaces that require load-bearing capacity, corrosion resistance and flame retardancy. Different resin systems suit different applications; please contact us to confirm the specific selection based on your actual working conditions.

Selection Guide

Selection mainly depends on media corrosiveness, load-bearing requirements and fire safety requirements: the phenolic type has a high limiting oxygen index and is suitable for applications with high requirements for low toxicity, high flame retardancy and fire safety; the vinyl type offers better corrosion resistance and is suitable for common acid and alkali environments. Please contact us for detailed specifications and quotations, and we will help match the resin type and grating structure.

Product Advantages

Assembled from pultruded profiles, the panels are lightweight, high-strength, corrosion-resistant and easy to cut and install on site, reducing later maintenance. The open-gap structure between profiles and cross rods provides both load-bearing capacity and drainage and ventilation, making it suitable for a variety of industrial environments.

Inquiry Guide

For specific information on the dimensions, resin type, load-bearing capacity and delivery time of Pultruded Grating HL-6020, please contact us. We will provide detailed specifications and quotations according to your working conditions.

Operating Environment

  • Pultruded FRP grating HL-6020 is built around pultruded I- and T-shaped bearing bars tied with solid pipe or bar connecting rods, a construction intended for walking surfaces where steel would corrode.
  • The phenolic MP-5 resin option is formulated for low-toxicity, high flame-retardant service, making it suitable for indoor and outdoor locations where fire safety is a priority.
  • Vinyl ester and other resin systems in the range are selected for continuous exposure to humid, chemical-laden or otherwise corrosive surroundings.
  • Typical working positions include platform walkways, stair treads and access covers in industrial plants; contact us with your site conditions for the full parameter list.