玻璃钢模塑格栅38*38H25
发起询价
欢迎询价。
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*38*25(mm)
Panel size available:
1220*4010,1220*3660,1524*4010,
997*3012,915*3050Bidirectional force.
Bearing bar thickness (Top/Bottom):6.4/5.0
Bearing bar center:38
Opea Area:68%
Approx Weight:12.3kg/㎡

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Application Scenarios
FRP molded grating 38*38H25 is widely used for working platforms, walkways, stair treads and trench covers in chemical, petroleum, power, wastewater treatment, marine engineering and other fields. Its corrosion resistance, slip resistance and light weight make it an ideal choice for wet and corrosive environments.
Selection Guide
When selecting, please consider load requirements, corrosive environment, fire resistance requirements and installation method. Different resin types (such as orthophthalic, isophthalic, vinyl ester and bisphenol A) and additives (such as ATH and PR) can provide different corrosion resistance and flame-retardant performance. Please contact us for detailed specifications and selection advice.
Product Advantages
FRP molded grating offers excellent corrosion resistance, high strength, light weight, slip resistance, insulation and long service life. Its 38*38mm mesh and 25mm thickness design balances load bearing and open area, making it easy to install and maintain.
Inquiry Guide
For more information on the technical parameters, price and customization services of FRP molded grating 38*38H25, please contact us for detailed specifications and a quotation. Our professional team will help you select a suitable solution.
Operating Environment
- Molded FRP grating is suited to both indoor and outdoor installations, including platforms, walkways and stair treads in industrial plants, water treatment facilities and chemical processing areas.
- The unsaturated polyester resin and glass fiber construction resists corrosion from acids, alkalis, salts and many other chemical media, making it suitable for wet, humid or splash-exposed locations.
- With no metal content, the grating does not rust and requires no painting, so it performs in coastal and other environments where steel would deteriorate.
- For elevated temperatures or unusually aggressive chemical service, contact us with the specific medium and conditions so the appropriate resin grade can be recommended.