玻璃钢模塑格栅25*152H38

玻璃钢模塑格栅25*152H38

价格面议

发起询价


欢迎询价。

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

25 152 H38

25*152*38(mm)

Panel size available:

1220*3660,1220*2440,915*3050 Length stress      

Bearing bar thickness (Top/Bottom):9.0/6.5

Bearing bar center:25

Open Aera:63%

Approx Weight:22.5kgs/m²

25 152 H38

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly. 

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 25*152 H38 is suitable for walkways, platforms, trench covers and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity, and is commonly used in chemical, water treatment, power and marine engineering environments. To confirm whether it fits your specific scenario, please contact our technical team for discussion.

Selection Guide

When selecting, it is necessary to consider whether the resin system (such as orthophthalic, isophthalic, vinyl ester or bisphenol A type), grating thickness and mesh size match the load and media conditions, and you may also confirm whether flame retardancy, a slip-resistant surface or special colors are required. As specific working conditions and parameters are involved, we recommend you provide your usage environment information so that we can assist with specification selection.

Product Advantages

This molded grating uses unsaturated polyester resin as the matrix with glass fiber reinforcement, offering light weight and high strength, chemical corrosion resistance, insulation and non-magnetic properties, and easy cutting and installation, with an optional slip-resistant surface treatment. Compared with traditional metal grating, it supports longer-term use and maintenance in humid or corrosive environments, with specific performance depending on the resin and formulation.

Inquiry Guide

For detailed specifications, suitable solutions and commercial terms for FRP molded grating 25*152 H38, please contact us for detailed specifications and a quotation. Please let us know your application environment, required dimensions and quantity, and we will provide selection recommendations and product information as soon as possible.

Operating Environment

  • FRP molded grating with a 25×152 mm mesh and 38 mm depth is used in outdoor walkways, platforms and stair treads where UV exposure and weathering are continual, so the isophthalic or bisphenol-A resin options are chosen for their resistance to sunlight degradation.
  • In industrial plants, this grating is installed over chemical process areas, drainage channels and wash-down zones, where the unsaturated polyester resin system and ATH filler resist splashes of acids, alkalis and solvents that would corrode steel.
  • Because the fiberglass reinforcement does not rust, the grating is suitable for humid, condensation-prone and coastal atmospheres, including indoor pits and outdoor structures with frequent wetting.
  • For high-temperature service or fire-sensitive locations, the phenolic resin grade listed in the resin table offers low toxicity and high flame retardant properties, suited to enclosed environments where smoke emission is a concern.