玻璃钢模塑格栅 38*38H15

玻璃钢模塑格栅 38*38H15

价格面议

发起询价


欢迎询价。

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38*38H15

38*38*15(mm)

Panel size available:

1220*3660,1220*4000,1220*2440,

921*3055,1264*4010 Bidirectional force.     

Bearing bar thickness (Top/Bottom):6.0/5.0

Bearing bar center:38

Open Aera:78%

Approx Weight:7kgs/m²

Liner load

Liner load(units:mm)

 Span in (mm)

Load in kn/m of widht
(concentrated)

Maximum
 
Recommended

Apparent E1*10^6 N-mm^2/m

4002.8197.14
6007.9138.55
Uniform load

Uniform load(units:mm)

Span in (mm)

Load in kn/sqm
(uniformed)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4000.71007.14
6003.0458.55
8008.9269.02
38*38H15

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

38*38H15
38*38H15
38*38H15

Application Scenarios

FRP molded grating 38*38H15 is suitable for walkways, trench covers, operating passages and equipment fencing where slip resistance, corrosion resistance and load bearing are required. Its mesh structure allows liquids and debris to pass through, and it is commonly used in chemical, water treatment, electroplating, marine engineering and general industrial platforms. For suitability under specific operating conditions, please contact us to confirm.

Selection Guide

During selection, the resin type, grating thickness and mesh size should be determined based on load requirements, span, support method, and the corrosive media and fire protection requirements of the service environment. On this page, 38*38H15 indicates the mesh and height designation; different resin systems offer different emphasis on corrosion resistance or flame retardancy. Please share your operating conditions with us so that we can recommend a suitable configuration.

Product Advantages

Molded grating is integrally formed from unsaturated polyester resin and glass fiber in custom molds, combining light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut, install and maintain. The surface can be made as anti-slip gritted or smooth to suit different walking and drainage requirements. Overall performance varies with the selected resin and filler system.

Inquiry Guide

For specific specifications, resin selection and commercial terms for FRP molded grating 38*38H15, please contact us to obtain detailed specifications and a quotation. Please provide your service environment, load and dimensional requirements, and we will match a solution for you as soon as possible.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送