玻璃钢模塑格栅38*152H38

玻璃钢模塑格栅38*152H38

价格面议

发起询价


欢迎询价。

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38 152 H38

38*152*38(mm)

Panel size available:

1220*3660,1220*2440,915*3050 Length stress      

Bearing bar thickness (Top/Bottom):8.0/6.0

Bearing bar center:38

Open Aera:67%

Approx Weight:15.92kgs/m²

Liner load

Liner load(units:mm)

Deflcvtion

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

Span( mm)

75150300450600750

Load

300<0.25<0.250.250.510.510.7612628
450<0.250.250.761.021.521.789946
6000.250.761.522.293.053.818233
7500.761.272.794.065.336.67040
9001.022.294.326.648.6410.96146
10501.523.36.69.91------5439
12002.294.839.65---------5141
Uniform load

Uniform load(units:mm)

Deflcvtion

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

Span( mm)

350450750100015002500

Load

300<0.25<0.25<0.250.250.250.5141358
450<0.250.250.510.761.021.7826962
6000.511.021.271.782.794.5721716
7501.032.033.054.066.35---18446
9002.544.066.18.1312.2---13420
10504.577.1110.7---------10180
12007.8711.9------------8418
38 152 H38

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRPgrating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 38*152 H38 is suitable for operating platforms, walkways, trench covers and stair treads in petrochemical, power, wastewater treatment, marine engineering and other fields. Its corrosion resistance, light weight and high strength make it perform well in humid, acid and alkali corrosive environments.

Selection Guide

When selecting, factors such as load requirements, service environment (corrosive media, temperature) and safety needs (e.g., flame retardancy, anti-slip) should be considered. Different resin types (such as orthophthalic, isophthalic, vinyl ester, phenolic) provide different corrosion resistance and flame-retardant properties, and can be selected according to specific working conditions. Please contact us for detailed specifications and selection advice.

Product Advantages

FRP molded grating offers advantages such as light weight and high strength, corrosion resistance, anti-slip, insulation and maintenance-free operation, and colors and sizes can be customized on demand. Its unique mesh structure facilitates installation and cutting, making it suitable for various complex occasions.

Inquiry Guide

For more product information, technical parameters or quotations, please contact us at any time. We provide professional technical support and customization services. You are welcome to inquire.

Operating Environment

  • Molded FRP grating 38*152H38 is built for outdoor and indoor service in industrial plants, replacing steel grating where moisture and chemical attack shorten service life.
  • The isophthalic, vinyl ester and bisphenol-A polyester resin systems specified above suit continuous contact with acidic, alkaline and saline media in chemical processing, wastewater treatment and coastal installations.
  • The E-glass fiberglass reinforcement and ATH / PR filler loadings shown in the material table give the molded grid dimensional stability under humid and wet conditions, with resistance to rot and corrosion.
  • The phenolic resin grade (MP-5) in the raw material list is intended for low-toxicity, high flame-retardant areas such as tunnels, offshore platforms and enclosed spaces where fire safety is a priority.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送