玻璃钢模塑格栅25*100H25
发起询价
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




25*100*25(mm)
Panel size available:
1007*3007 Width stress
Bearing bar thickness (Top/Bottom):7.0/5.5
Bearing bar center:25
Open Aera:67%
Approx Weight:13kgs/m²

Liner load(units:mm)
Deflcvtion | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
Span( mm) | 75 | 150 | 300 | 450 | 600 | 750 | Load |
| 300 | 0.33 | 0.48 | 0.74 | 0.99 | 1.27 | 1.52 | 9942 |
| 600 | 0.86 | 1.73 | 3.45 | 5.18 | 6.91 | 8.64 | 4305 |
| 750 | 1.40 | 2.72 | 5.11 | 7.16 | 9.55 | 11.9 | 3589 |
| 900 | 2.41 | 4.72 | 8.18 | 12.4 | 16.5 | 20.6 | 3216 |

Uniform load(units:mm)
Deflcvtion |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
|---|---|---|---|---|---|---|---|
Span( mm) | 240 | 480 | 980 | 1450 | 2450 | 3650 | 4880 |
| 300 | 0.28 | 0.38 | 0.53 | 0.71 | 1.04 | --- | 1.91 |
| 600 | 0.91 | 1.85 | 3.68 | 5.54 | 9.22 | --- | 18.5 |
| 900 | 3.63 | 6.6 | 12.6 | 18.5 | --- | --- | --- |
| 1050 | 8.01 | 14.9 | --- | --- | --- | --- | --- |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP Molded Grating 25*100H25 is suitable for platforms, walkways, stair treads and trench covers in chemical, petroleum, power, marine engineering and other fields. Its corrosion resistance, slip resistance, light weight and high strength make it perform well in harsh environments such as humid and acid-alkali conditions.
Selection Guide
When selecting, consider load-bearing requirements, span, corrosive environment and safety level. 25*100H25 indicates a grating thickness of 25 mm and a mesh size of 100 mm. Different resin types (such as orthophthalic, isophthalic, vinyl ester, phenolic, etc.) can be selected according to specific needs to meet corrosion resistance or flame retardant requirements.
Product Advantages
FRP molded grating features light weight, high strength, corrosion resistance, slip resistance, insulation and maintenance-free performance, with a long service life and easy installation, effectively reducing long-term costs.
Inquiry Guide
For more detailed specifications or technical parameters of FRP Molded Grating 25*100H25, or to obtain a quotation, please contact us. We will provide you with professional technical support and customized services.
Operating Environment
- This FRP molded grating is built on unsaturated polyester resin, which supports use in both indoor and outdoor installations where moisture and humid air are present.
- The phenolic resin option (MP-5) provides low toxicity and high flame retardant properties, making it suitable for fire-sensitive environments.
- With its fiberglass reinforcement and resin matrix, the grating is appropriate for areas exposed to corrosive media, as the material resists chemical attack.
- Typical applications include walkways and platforms where the grating must withstand foot traffic and environmental exposure without losing structural integrity.