玻璃钢模塑格栅20*20H40

玻璃钢模塑格栅20*20H40

价格面议

发起询价


欢迎询价。

Genius FRP   

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber      

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type   

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

20 20 H40

20*20*40(mm)

Panel size available:

1007*4047,1007*3007 Bidirectional force.     

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:20

Open Aera:42%

Approx Weight:23.7kgs/m²

20 20 H40

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 20*20 H40 is suitable for platforms, walkways, trench covers and various operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity. It is commonly used in chemical, water treatment, power and marine engineering environments. Its open mesh structure facilitates drainage, ventilation and light transmission, and also makes on-site cutting and installation easier. For suitability in specific scenarios, please contact us to discuss and confirm.

Selection Guide

When selecting, we recommend first clarifying the corrosive medium, load-bearing requirements and installation method of the service environment, then confirming the grating mesh size, thickness and resin system accordingly. The resin types listed on this page each have different strengths in flame retardancy and corrosion resistance, and can be selected according to actual working conditions. Please contact us for detailed specifications and selection advice.

Product Advantages

Molded forming gives the grating good structural integrity and uniform fiber and resin distribution, offering light weight, high strength, corrosion resistance and slip resistance, with relatively low maintenance costs. The surface can be treated for slip resistance, and it is not prone to rusting over long-term use. For specific performance data, please contact us to request documentation.

Inquiry Guidance

For detailed specifications, resin options and commercial terms of FRP molded grating 20*20 H40, please contact us for detailed specifications and a quotation. Please inform us of the service environment and required quantity, and we will provide a tailored solution and sample support.

Operating Environment

  • The molded FRP grating is built from unsaturated polyester resin systems, including isophthalic, vinyl ester and bisphenol types, so the 20*20H40 panel is intended for locations where moisture and chemical splash are part of daily service.
  • Typical installations are outdoor walkways, platforms, stair treads and trench covers in plants, where the grating sees rain, sun exposure and wash-down rather than a controlled indoor climate.
  • Because the resin type can be selected (OFR, IFR, VEFR grades and the MP-5 phenolic type with high flame retardancy and low toxicity), the same 20*20H40 grating is used both in general industrial areas and in fire-sensitive zones.
  • Corrosive media such as acids, alkalis and salts are commonly present in these service areas; the bisphenol and vinyl ester resin options are chosen where such exposure is expected. Contact us for the full parameter list and the resin grade recommended for your specific environment.

立即联系我们,我们将有专业人员为您服务。