Product Category

产品详情

Genius FRP    

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Sand surface

Smooth surface

Antiskid groove surface

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 38mm
Open Area: 25%

Approx Weight (With three-core shoots): 16.7kg/m²

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

15030045075015003000

Load

450<0.250.250.250.511.022.297539
6000.250.510.511.022.034.066020
9000.511.271.783.056.3512.44023
12001.522.794.327.11------3010

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

4509501450240048509500

Load

450<0.250.250.250.511.022.0316494
6000.250.510.761.272.545.0812346
9001.272.293.565.8411.7---8247
12003.567.1110.7---------4929

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  


Application Scenarios

Pultruded Grating T-2515 is assembled from pultruded I/T-shaped load-bearing bars with solid tubes or rods as connecting rods. It is suitable for platforms, walkways, trench covers and various industrial operating surfaces that require load-bearing capacity, corrosion resistance and water/air permeability. For the load and span requirements of specific scenarios, please contact us to confirm the selection based on your working conditions.

Selection Guide

During selection, the resin system (such as orthophthalic, isophthalic, vinyl ester or phenolic, etc.), load-bearing bar specifications and grating gap can be matched to the service environment and load-bearing requirements; for highly corrosive or high fire protection requirements, the corresponding resin type can be given priority. Please provide the service environment, span and load conditions, and we will assist you in determining a suitable configuration.

Product Advantages

Pultruded grating uses continuous pultruded profiles as load-bearing units, with fibers continuously distributed along the load-bearing direction. It combines relatively high longitudinal strength, light weight and corrosion resistance, and its assembled structure facilitates cutting and on-site installation. The surface can be treated with anti-slip treatment, making it suitable for wet or slippery environments.

Inquiry Guide

If you need detailed specifications, resin and color options, supply forms and commercial terms for Pultruded Grating T-2515, please contact us for detailed specifications and quotations. Please inform us of the application scenario and quantity requirements, and we will provide you with selection suggestions and solutions as soon as possible.

Operating Environment

  • Built for outdoor walkways, platforms and stair treads, where the pultruded FRP bearing strips and rod connectors resist weather exposure without rusting.
  • Suitable for indoor plant service in humid or wet areas, since the fiberglass-reinforced profiles do not corrode like steel under moisture.
  • Recommended for chemically aggressive surroundings such as industrial floors and process areas, where the resin-rich pultruded surface tolerates splashes and fumes better than metal grating.
  • Contact us for the full parameter list, including the resin system best matched to your specific temperature and chemical exposure.