产品详情
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |
Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 38mm
Open Area: 40%
Approx Weight (With three-core shoots): 22kg/m²
Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.12 | 0.25 | 0.51 | 0.76 | 1.52 | 2.79 | 26215 |
| 600 | 0.29 | 0.51 | 1.02 | 1.78 | 3.05 | 5.84 | 19661 |
| 900 | 1.02 | 1.27 | 2.29 | 5.32 | 9.38 | 17.8 | 12705 |
| 1200 | 2.95 | 3.59 | 5.57 | 9.4 | 19.1 | 38.9 | 9086 |
Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.25 | 0.45 | 0.76 | 1.67 | 2.42 | 4.83 | 114645 |
| 600 | 0.61 | 1.18 | 2.32 | 4.59 | 5.96 | 9.62 | 64506 |
| 900 | 1.92 | 3.79 | 6.33 | 11.2 | 15.5 | --- | 27757 |
| 1200 | 4.96 | 9.64 | --- | --- | --- | --- | 14905 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories
Application Scenarios
Pultruded Grating I-4015 is assembled from pultruded "I"-shaped load-bearing bars with solid tubes or rods as connecting rods. It is suitable for platforms, walkways, trench covers and various industrial operating surfaces where load-bearing capacity and corrosion resistance are required. In chemical, water treatment, electroplating, marine and general corrosive media environments, different resin systems can be selected according to specific working conditions. Please contact us to describe your operating environment so we can confirm a suitable solution.
Selection Guide
When selecting, we recommend first clarifying the medium type and concentration, ambient temperature, load form and installation support span, then choosing the resin type (such as phenolic, vinyl ester, etc.) as well as grating thickness and load-bearing bar spacing accordingly. Different resins have different emphases in flame retardancy and corrosion resistance. Please contact us for specific specifications and load-bearing data.
Product Advantages
Pultruded grating uses continuously pultruded profiles as load-bearing units. It features light weight and high strength, corrosion resistance, non-conductivity and maintenance-free operation, is easy to cut and install on site, and can reduce later maintenance costs. Its surface can be made anti-slip to improve walking safety. For specific performance details, please contact us for more information.
Inquiry Guide
If you need to learn about the detailed specifications, resin options, load-bearing capacity and quotation of Pultruded Grating I-4015, please contact us and provide your operating conditions and size requirements. We will recommend a suitable solution and provide a quotation.