Product Category

绿盟GB压实型不旋转钢丝绳19X7 (6/1)


Contact us for a quotation

产品详情

Product Details

The 19x7 compacted non-rotating wire rope is available in both galvanized and non-galvanized versions, and there are also 17x7 and 18x7 specifications. To further improve flexibility and other performance characteristics, we also offer specifications such as 32X7, 35X7 and 37X7.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Engineering Applications  

  • Offshore crane wire rope

  • Deck crane wire rope

  • Pillar crane wire rope

  • Lifting slings

  • Main hoist wire rope

  • Sling

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Diameter

Weight

(1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa) 

mm

kg/m

KN

Kg

KN

Kg

120.6391.7934910210388
130.741081097212012191
140.861251272513914139
150.991431460815916231
161.131631662118118467
181.432062103522923373
201.762552597028328855
222.133083142334234915
242.533673739640741551
262.974304388947848765
283.454995090155456556
303.965735843263764924


General engineering wire rope

   Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 in various specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also supply premium special wire ropes.

Most wire ropes work under demanding conditions and must have resistance to crushing, bending fatigue and wear. All our wire ropes strive to achieve a high level of performance to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged ends and wedge sockets, as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.

Selection Guide

When selecting, first clarify the rated load of the lifting equipment, the pulley and drum diameters, the operating environment (such as offshore, humid or corrosive conditions) and the required safety factor, then determine the suitable specification by referring to the diameter and minimum breaking load comparison table. Different surface treatments (bright or galvanized) and constructions (such as 17x7, 18x7, 32x7, etc.) suit different applications. We recommend informing us of your specific working conditions so our technical staff can help match the right specification.

Product Advantages

This 19x7 compacted non-rotating wire rope uses a compacting process and has a tight structure, offering good anti-rotation performance during lifting and hoisting, which helps reduce load swing. The product can be supplied with bright or galvanized surface treatment as required and complies with GB/T 20118-2006, making it suitable for offshore cranes, deck cranes, pillar cranes and main hoisting applications.

Inquiry Guidance

For specific specifications and quotations covering different diameters, surface treatments, and 1770 MPa or 1960 MPa strength grades, please contact us for detailed technical documents and commercial proposals. We can recommend a suitable construction based on your working conditions and confirm supply and delivery arrangements.